GA-60X1A
Herchy
| kasadiaan: | |
|---|---|
| kuantitas: | |
GA-60X1A Karét Silikon Tahan Panas (250 Sareng 300 OC) (HCR)
Aplikasi: cocog pikeun ngahasilkeun suku cadang mobil, cots tahan panas, segel tahan panas sareng produk sanésna.
Fitur konci: résistansi panas anu saé sareng kakuatan mékanis, lulus auténtikasi RoHS, REACH, sareng FDA.
Uji: 1% agén curing (50% némpelkeun DBPMH dina karét silikon), 175 ° C x 5min x 15MPa.
| 250 derajat Parameter Produk | |||||
| produk | GA-6041A | GA-6051A | GA-6061A | GA-6071A | |
| Penampilan | Tembus cahaya | ||||
| Williamplastisitas | 150 | 200 | 240 | 240 | |
| Teu karasa (ShoreA) | 40 | 50 | 60 | 70 | |
| Kapadetan (g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Kakuatan tegangan (MPa) | 8.5 | 9 | 9.5 | 9 | |
| Elongation(%) | 700 | 600 | 500 | 400 | |
| Kakuatan cimata (kN/m) | 15 | 20 | 25 | 25 | |
| hawa sepuh 250 ℃ x70H | Teu karasa | 45 | 54 | 64 | 75 |
| Kakuatan tegangan | 6.2 | 7.3 | 7.5 | 6.5 | |
| Elongation | 380.0 | 300.0 | 280.0 | 200.0 | |