U teng mona: Lehae » Litharollo » Litharollo » Litharollo tsa ho thibela metsi ha ho etsoa rabara

Litharollo tsa ho hanyetsa metsi ka mekhoa ea rabara

I. Rabara ea tlhaho

Ho kenngoa ha metsi: Ho kenngoa ha metsi ka rabara ea tlhaho ho fapana le ho kopana ha latex, mofuta oa 'preservative le coagulant', khatello ea ho hlatsoa le maemo a ho omisa nakong ea ho etsa rabara, kahoo ho na le phapang e totobetseng ea ho kenngoa ha metsi a mefuta e fapaneng ea lihlahisoa.

II. Rabara ea styrene butadiene

Ho monya metsi: ho ts'oana le rabara ea tlhaho.

III. Rabara ea Butadiene

Ho kenngoa ha metsi a tlaase: Mocheso oa metsi oa rabara ea butadiene o tlaase ho feta oa rabara ea styrene butadiene le rabara ea tlhaho, e ka etsang rabara ea butadiene e sebelisetsoang ho thibela terata ea motlakase le lihlahisoa tse ling tsa rabara tse hlokang ho thibela metsi.

IV. Butyl rabara

Rabara ea Butyl e na le ho kenella ha metsi ka tlase haholo, ho hanyetsa metsi ho matla ka mocheso o akaretsang, 'me sekhahla sa ho monya metsi ka mocheso oa kamore ke makhetlo a 10-15 ho feta liraba tse ling. Ts'ebetso ena e ntle haholo ea rabara ea butyl ke tlatsetso ea bohlokoa molemong oa ho kenya motlakase. Rabara ea Butyl e matlafalitsoeng ka carbon black and vulcanized with resin e ka fumana ts'ebetso e tlaase ea ho monya metsi tlas'a mocheso o phahameng le maemo a nako e telele a ho pepeseha. E le ho nolofalletsa rabara ea butyl ho pepesehela metsi kapa mocheso o phahameng ka nako e telele, lintlha tse latelang li lokela ho etsoa ka molao-motheo:

1, filler e lokela ho ba e seng hydrophilic le meta-electrolytic.

2, lintho tse qhibilihang ka metsing tsa sistimi ea vulcanization li lokela ho ba tse nyane ka moo ho ka khonehang

3, Maemo a matlafatsang a khethiloeng le maemo a vulcanization a lokela ho etsa hore rabara e hlasetsoeng e be le modulus e phahameng ea elastic le lisebelisoa tse ling tsa 'mele.

V. Ethylene propylene rabara

Ho hanyetsa metsi a chesang le mouoane oa metsi. Ethylene propylene rabara e na le khanyetso e ntle ea mouoane, e betere ho feta ho hanyetsa mocheso. Ho hanyetsa ha eona ho matla ho feta rabara ea butyl le rabara e akaretsang. Ethylene propylene rabara e boetse e na le khanyetso e ntle ho metsi a chesang, empa e amana haufi-ufi le tsamaiso ea vulcanization e sebelisoang. Tšebeliso ea peroxide le tsamaiso e sebetsang ea vulcanization ea ethylene propylene rabara vulcanization rabara peroxide tshebetso e molemo haholo ho feta sulfur vulcanization ea rabara ea ethylene propylene kapa rabara ea butyl, empa sulfur vulcanization ea ethylene propylene rabara vulcanization rabara peroxide tshebetso ea rabara e mpe haholo ho feta sulfur vulcan.

VI. Rabara ea Neoprene

Ho hanyetsa metsi ho molemo ho feta rabara e 'ngoe ea maiketsetso, ho tiea ha khase ho latela rabara ea butyl.

Ho lokisoa ha rabara e sa keneleng metsi ea neoprene, ho lokela ho ela hloko khetho ea sistimi ea vulcanization le filler. Vulcanization tsamaiso e molemo ka ho fetisisa ho sebelisa tsamaiso ea lead oxide, qoba ho sebelisa magnesium oxide, zinc oxide system. Lead oxide dosage likarolong tse 20 kapa ka tlaase ho moo, ho na le karolo ea ho ntlafatsa ho hanyetsa metsi, empa tekanyo e ngata haholo empa ha e sebetse. Ha u sebelisa lead sulfide, khetho e ntle ka ho fetisisa ea ho matlafatsa carbon black, carbon black ka mokhoa oa slot carbon black e molemo, mokhoa oa sebōpi oa carbon black ke oa bobeli. Inorganic filler e molemo ka ho fetisisa ho sebelisa calcium silicate, e lateloa ke barium sulfate, letsopa, joalo-joalo Lisebelisoa tsohle tsa hydrophilic ha lia lokela ho sebelisoa. Hape ha ua lokela ho sebelisa sulfur vulcanization. Ts'ebetso ea rabara e hanyetsanang le metsi hangata e fokola, ho lokela ho hlokomeloa ha ho sebetsoa.

VII. Rabara ea nitrile

Ho hanyetsa metsi ho molemo: ka keketseho ea li-acrylonitrile, ho hanyetsa metsi ho mpefala.

VIII. Rabara ea silicone

Hydrophobicity: matla a bokaholimo ba rabara ea silicone e tlase ho feta lisebelisoa tse ngata tsa manyolo, ka hona, e na le monyetla o tlase oa mongobo, ho qoelisoa ka nako e telele ka metsing, sekhahla sa ho monya metsi se ka bang 1% feela, thepa ea 'mele le ea mochini ha e fokotsehe, ho hanyetsa hlobo ho lokile.

IX. Rabara ea Fluorine

Ts'ebetso e tsitsitseng bakeng sa metsi a chesang. Ho na le khanyetso e babatsehang ea mocheso o phahameng oa mouoane.

Fluorine rabara ka karolo ea ho tsitsa ha metsi a chesang, eseng feela ho itšetlehile ka mofuta oa rabara e tala ka boeona, empa hape e khethoa ke thepa ea rabara e nang le. Bakeng sa rabara ea fluorine, ts'ebetso ena e itšetlehile haholo ka tsamaiso ea eona ea vulcanization. Peroxide vulcanization system e betere ho feta amine, bisphenol AF mofuta oa vulcanization system. 26 mofuta oa fluoroelastomer o sebelisang ts'ebetso ea rabara ea amine vulcanization e mpe ho feta rabara e akaretsang ea maiketsetso joalo ka rabara ea ethylene propylene, rabara ea butyl. Rekere ea mofuta oa G-fluorine e sebelisang sistimi ea vulcanization ea peroxide, likhokahano tse hokahantsoeng tsa rabara e senyehileng ho feta amine, mofuta oa bisphenol AF mofuta oa vulcanized rubber cross-linked link to hydrolysis stability is better.

X. Polyurethane

E 'ngoe ea mefokolo e hlahelletseng ea polyurethane: ho hanyetsa ha hydrolysis ho futsanehile, haholo-holo ka mocheso o phahameng hanyenyane kapa ho ba teng ha asiti le alkali media hydrolysis ka potlako.

XI. Chlorine ether rabara

Homopolymerized chloroether rabara le rabara ea nitrile e na le khanyetso ea metsi e ts'oanang, khanyetso ea metsi ea chloroether ea copolymerized pakeng tsa rabara ea nitrile le rabara ea acrylate. Sebopeho se na le tšusumetso e kholo ea ho hanyetsa metsi, e nang le PB3O4 ho hanyetsa metsi a rabara ho molemo, e nang le MGO ho hanyetsa metsi ho mpefala haholo, ho ntlafatsa tekanyo ea vulcanization ho ka ntlafatsa ho hanyetsa metsi.

XII. Chlorosulfonated polyethylene rabara

Cross-linking chlorosulfonated polyethylene rabara e nang le epoxy resin kapa likarolo tse fetang 20 tsa lead monoxide e ka etsa hore rabara e hlasetsoeng e be le khanyetsano e ntle ea metsi. Filler e sebelisitsoeng ho kenyelletsa calcium carbonate, setlolo se tloaelehileng sa ho tlatsa barium sulfate, letsopa le thata le ho phatloha ha carbon black ho loketse haholoanyane. Ho phaella moo, e le ho etsa hore rabara e nang le vulcanized e fumane khanyetso e ntle ea metsi, vulcanization e haufi ke ea bohlokoa haholo.

Bakeng sa ho pepeseha ha nakoana ka metsing kapa lihlahisoa tsa nako e khuts'oane, hangata barium oxide e fumaneha joalo ka ntho e senyang, joalo ka rabara ea chlorosulfonated polyethylene e nang le likarolo tse ka bang 5 tsa oli ea silicone, ebe e kopantsoe le rabara ea magnesium oxide vulcanization ka sekhahla sa ho ruruha ha metsi le eona e nyane haholo.

XIII. Acrylate rabara

Hobane sehlopha sa ester se bonolo ho hydrolyze, ho etsa rabara ea acrylate ka sekhahla sa ho ruruha ha metsi se seholo, rabara ea mofuta oa BA ka 100 ℃ metsi a belang ka mor'a hore boima ba 72h bo fumanehe ka 15-25%, ho atolosoa ha molumo oa 17-27%, ho hanyetsa mouoane ho mpefala.


LIEKETSENG POTLAKO

LIHLAHISO TSA RONA

MOKHOA OA PUISANO

Eketsa: No.33, Lane 159, Taiye Road, Setereke sa Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sebaka sa marang-rang |   Leano la Lekunutu | Tšehetso Ka Leadong.