U mona: Hae » Litaba » Ts'ebeliso ea Ultrafine e sebetsang Litaba ea Zinc Oxide ho Hose Rubber

Kopo ea Ultrafine e sebetsang ea Zinc Oxide ho Hose Rubber

Maikutlo: 0     Mongoli: Nako ea Phatlalatsa: Nako ea Phatlalatsa: 2023-08-15: Sebaka

Botsa

Zinc Oxide e sebelisoa haholo e le moemeli ea sebetsang ka har'a lihlahisoa tsa rabara, tse ka potlakisang lebelo la Vulcanization, 'me ke karolo ea bohlokoa ea silcanlization ea lihlahla. Ha e bapisoa le li-zinc tse tloaelehileng tsa Zinc tse tloaelehileng tsa Zinc oxide. Ka hona, ho nka sebaka se tloaelehileng sa zinc ka sebopeho sa rabara se ka fokotsa tlhahlobo ea sona ntle le rabara ea Vulcanization ea rabara.

 

Liteko tsa laboratori

 

Ha litekanyetso tsa Zinc tse sebetsang  li ne li eketseha ho tloha ho 50% ho isa ho 90%, nako ea ho senya bakeng sa e matla . rabara

Nako ea ho etsa nako ea ho senya nako ea Vulcanization (T10) le nako e ntle ea e ile ea eketseha ka keketseho ea litekanyetso, 'me ho ile ha Vulcanization  fumaneha thepa e ntlehali ea rabara. Ho thata ha lingoliloeng tsa rabara ha li fetole haholo le keketseho ea tekanyetso e sebetsang ea Zinc Oxide.

 

Netefatso ea Batch

 

Ha litekanyetso tsa Zinc tse sebetsang li hlahisa 70% ea li-axide tse tloaelehileng O khethile karolelano, o sebelisa tlhahlobo e teteaneng, ho etsa tlhahlobo e kholo ea papiso, liphetho li bontšoa tafoleng ea 3. Liphetho tsa liteko li bonts'a hore litekanyetso tsa zinc li bonts'a

ke 70% ea matla a patsi ea zinc e tloaelehileng e phahame ho feta ea lits'ila tse tloaelehileng

 

Ho kopanya

Ultrafine e sebetsang ea zinc oxide e bonolo ho fofa ha e kopanya ka lebaka la boholo bo bonyenyane le boima bo bobebe. Ho kopanya le Mofumahali ho ka nka taolo ea mokhoa o kopanyang, e sebetsang ka kamoreng e ncha, ebe u lahla lisebelisoa tse ling bakeng sa ts'ebetso

 

Ho fetotsoe

T10 ea Zinc oxide e sebetsang  e telele ho feta palo ea zinc e tloaelehileng, e leng molemo ho e ntlafatsang ea hose le ho fokotsa bothata ka lebaka la ho phahama ka nako ea mocheso nakong ea mocheso. Tlhahiso e sebetsang e bontšitse hore rabara ea rabara e sebelisa ts'ebetso e sebetsang ea Zinc e sebetsang, ts'ebetso ea ts'ebetso ea Exercud e ntle. Ho fetotsoe

Taolo ea Mechine ea Mechine: Mocheso oa Mocheso 70 ± 5 , mocheso oa 'mele 50 ± 5 , Screw Movie 40 ± 5 .

 

Vulcanization

Ts'ebeliso ea li-oxide tse sebetsang tsa Zinc le tse tloaelehileng tsa Zinc tse tloaelehileng li batla li lekana le mocheso oa VulCanization le nako e ka sebelisoa ts'ebetsong ea mantlha.

 

Litšenyehelo

Theko ea zinc e sebetsang e phahame ho feta oxide e tloaelehileng ea Zinc e tloaelehileng, empa litekanyetso li ka fokotsoa, ​​ho ea ka tlhahlobo, foromo ea hose e ka sebelisoa 70% ea litekanyetso. Litsenyehelo tse felletseng li tla ba tlase.

 

Sephetho

 

.

(2) Ultrafine ultrafine e sebetsang  ea zinc e sebelisoa hose, ts'ebetso ea ts'ebetso e tloaelehile. Ka lebaka la nako e telele ea T10, ts'ebetso ea Anti-scorch e ntle, e iphumanela ho iphetola.

(3) Ts'ebeliso ea tšebeliso ea ultrafine e sebetsang ea zinc e ka fokotsa litšenyehelo tsa rabara.


Lihokela tse potlakileng

Lihlahisoa tsa rona

MOKHOA OA PUISANO

Kenya: No.33, Lane 159, Taiye Business, Setereke sa Fengxian, Shanghai
Tel / Whatsapp / Skype: + 86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co, Ltd. Sitemap |   Leano la Lekunutu | Ts'ehetso ea Phelana.