| Loaʻa: | |
|---|---|
| Nui: | |
Ethylene Propylene Rubber – EPDM/EPM
ʻO nā pono hana nui o EPDM penei.
(1) ʻO ke kumukūʻai kiʻekiʻe o ka hana, me ka nui o ka lāʻau maka o ka 0.86-0.90g/cm3 wale nō, ʻo ia ka māmā maʻamau o ka lāʻau maʻamau me ka nui o ka ʻōpala maka; a hiki ke omole ia i na mea nui e hoemi ai i ke koina o ke kalapa.
(2) ʻO ke kūpaʻa ʻelemakule maikaʻi loa, ka pale ʻana i ka wā, ka pale ʻana o ka ozone, ka pale ʻana o ka lā, ka pale ʻana i ka wela, ka pale ʻana i ka wai, ke kū ʻana o ka mahu wai, ka pale ʻana o UV, ka pale ʻana i ka radiation a me nā mea kahiko ʻē aʻe. Ke hoʻohana ʻia ʻo EPDM me ka hui pū ʻana me nā rubbers diene unsaturated e like me NR, SBR, BR, NBR, CR, etc., hiki iā ia ke hana ma ke ʻano he antioxidant polymer a i ʻole anti-aging agent.
(3) Ke kū'ē kemika maikaʻi loa, ka waikawa, ka alkali, ka mea holoi, nā aila holoholona a me nā mea kanu, ka waiʻona, ketone, etc.; ʻoi aku ka maikaʻi o ke kūpaʻa wai, ka wai wela nui, ke kū ʻana o ka mahu wai; pale ʻaila polar.
(4) Hana maikaʻi i ka insulation, ka nui resistivity 1016Ω-cm, breakdown voltage 30-40MV/m, dielectric mau (1kHz, 20℃) 2.27.
(5) ʻO ka laulā wela o ka hana, ka mahana hana liʻiliʻi -40-60 ℃, hiki ke hoʻohana no ka manawa lōʻihi ma lalo o 130 ℃.
Hoʻokuʻu aku ʻo Hirsch Rubber i ka EPDM/EPM i 15 mau ʻāina me ʻAmelika Hui Pū ʻIa, Russia, Brazil, Argentina, South Korea, Kelemānia, Italia, Sepania, Australia, a me India.
Ethylene Propylene Rubber-EPDM/EPM
| Herchy | Mooney viscosity | Mooney viscosity | Mooney viscosity | Ethylene maʻiʻo | ʻIke ENB | Hoʻonui-ʻaila maʻiʻo | Palapala noi | ʻAno |
| Papa |
ML(1+4)100 ℃ | ML(1+4)125 ℃ | ML(1+4)150 ℃ | wt% | wt% | PHR | ||
| S501A | 44 | [30] | 53 | 4.1 | Nā huahana hoʻoheheʻe ʻia; | Haʻahaʻa Mooney viscosity; ʻO ka wai maikaʻi; Kū'ē wela ha'aha'a; |
||
| S505A | 45 | [29] | 55 | 9.4 | Nā huahana paʻakikī kiʻekiʻe | Haʻahaʻa Mooney viscosity; ʻO ka wai maikaʻi; Maikaʻi ENB kiʻekiʻe; wikiwiki ho'ōla wikiwiki; Kū'ē wela ha'aha'a; |
||
| S537-3 | 35 | 57 | 2.3 | ʻO loko o loko; Kāma; Nā ʻāpana mīkini hana | Kūleʻa wela kiʻekiʻe; Pale wela haʻahaʻa; |
|||
| S537-2 | 40 | 57 | 3 | ʻO loko o loko; Nā ʻāpana mīkini hana | Kūleʻa wela kiʻekiʻe; Pale wela haʻahaʻa; |
|||
| S512F | 63 | 69 | 4.5 | Hose; Nā ʻāpana hoʻopaʻa puka a me ka puka makani; Huahana Extrusion; | ʻO ka nui o ka ethylene; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi |
|||
| S5890F | [87] | 64 | 68 | 5.5 | Hose; Hoʻopaʻa sila paʻa; | Hoʻopiha kiʻekiʻe ; |
||
| S552 | 84 | 58 | 4.1 | Hose; Hoʻopaʻa paʻa paʻa; Gasket; Nā huahana ʻoihana; | ʻOi aku ka maikaʻi o ka hana ʻana ; Ke kūpaʻa haʻahaʻa haʻahaʻa ; Nā waiwai mechanical kiʻekiʻe |
|||
| S552-1 | 84 | 58 | 5.7 | Hose; Hoʻopaʻa paʻa paʻa; Nā huahana ʻoihana; | ʻOi aku ka maikaʻi o ka hana ʻana ; Ke kūpaʻa haʻahaʻa haʻahaʻa ; Nā waiwai mechanical kiʻekiʻe ; |
|||
| S553 | [98] | 72 | 62 | 4.5 | ʻO nā pani pani puka a me ka puka makani; Waterproof; | Kiʻekiʻe Mooney viscosity ; Hoʻopiha kiʻekiʻe ; Ke kūpaʻa haʻahaʻa haʻahaʻa ; Nā waiwai mechanical kiʻekiʻe; |
||
| S5206F | [84] | 81 | 60 | 8.5 | Hōʻike puna ;Nā ʻāpana hū; | Kiʻekiʻe Mooney viscosity; kiʻekiʻe ENB maʻiʻo; wikiwiki hoʻōla wikiwiki; kiʻekiʻe mechanical waiwai; |
||
| S5527F | [109] | 81 | 60 | 8.5 | Hōʻike puna ;Nā ʻāpana hū ; Nā huahana rebound kiʻekiʻe; | Hoʻopiha kiʻekiʻe ; Kiʻekiʻe Mooney viscosity ; Maikaʻi ENB kiʻekiʻe ; Ka wikiwiki hoʻōla wikiwiki ; Nā waiwai mechanical kiʻekiʻe; |
||
| S6090WF | 53 | 70 | 5.7 | 50 | Nā huahana paʻakikī haʻahaʻa; Hose; Hoʻopaʻa i ka puka mīkini holoi; ʻO ke kaula uwea kaʻa; Nā huahana kiʻekiʻe kiʻekiʻe; Nā waiwai mechanical kiʻekiʻe | Maʻiʻo ethylene kiʻekiʻe ; Kiʻekiʻe Mooney viscosity ; Nā waiwai mechanical kiʻekiʻe ; Ka waiwai hana maikaʻi loa; |
||
| S600WF | 61 | [41] | 72 | 4 | 100 | Nā huahana haʻahaʻa paʻakikī | Hoʻopiha kiʻekiʻe ; Nā waiwai mechanical kiʻekiʻe ; Waiwai hoʻoponopono maikaʻi loa; |
|
| S7486F | 92 | 67 | 60 | 9 | Hōʻike puna; | Haʻahaʻa ethylene maʻiʻo; kiʻekiʻe ENB maʻiʻo; wikiwiki ho'ōla wikiwiki; |
||
| S6075WF | 50 | 60 | 4.7 | 75 | Nā huahana paʻakikī haʻahaʻa | Haʻahaʻa ethylene maʻiʻo; kiʻekiʻe Mooney viscosity; maikaʻi hoʻoili waiwai; haʻahaʻa haʻahaʻa wela pale; |
| Herchy | Mooney viscosity | Mooney viscosity | Mooney viscosity | Ethylene maʻiʻo | ʻIke ENB | Hoʻonui-ʻaila maʻiʻo | Palapala noi | ʻAno |
| Papa | ML(1+4)100 ℃ | ML(1+4)125 ℃ | ML(1+4)150 ℃ | wt% | wt% | PHR | ||
| J-2070 | 44* | 57.8 | 1.9 | ʻO loko o loko; Kāma; Nā ʻāpana mīkini hana | Pale wela kiʻekiʻe | |||
| J-2080 | 53 | 62 | 2 | ʻO loko o loko; Kāma; Nā ʻāpana mīkini hana | Kū'ē wela ki'eki'e | |||
| 3062E | 41 | 68.5 | 3.9 | 20 | Nā Huahana Hoʻoheheʻe Injection; Hose; Nā ʻāpana hoʻopaʻa puka a me ka puka makani; Huahana Extrusion; | ʻO ka nui o ka ethylene; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi |
||
| J-3060P | 45 | 68.5 | 4 | Hose; Nā ʻāpana hoʻopaʻa puka a me ka puka makani; Huahana Extrusion; | ʻO ka nui o ka ethylene; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi |
|||
| J-3080 | 70 | 68.5 | 4 | Hose; Nā ʻāpana hoʻopaʻa puka a me ka puka makani; Huahana Extrusion; | ʻO ka nui o ka ethylene; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi |
|||
| J-3080P | 70 | 68.5 | 4 | Hose; Nā ʻāpana hoʻopaʻa puka a me ka puka makani; Huahana Extrusion; | ʻO ka nui o ka ethylene; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi |
|||
| J-3092E | 60 | 57.2 | 4.6 | 20 | Hose; Nā ʻāpana hoʻopaʻa puka a me ka puka makani; Huahana Extrusion; | ʻO ka nui o ka ethylene; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi |
||
| 4045 | 45 | 52 | 7.7 | ʻO nā huahana paʻakikī kiʻekiʻe ; ʻaoʻao ʻaoʻao o ka pā; | Haʻahaʻa Mooney viscosity; ʻO ka wai maikaʻi; Maikaʻi ENB kiʻekiʻe; wikiwiki ho'ōla wikiwiki; Kū'ē wela ha'aha'a; |
|||
| J-4090 | 65 | 52.5 | 7.7 | ʻaoʻao ʻaoʻao huila; | Maikaʻi ENB kiʻekiʻe; wikiwiki ho'ōla wikiwiki; Kū'ē wela ha'aha'a; |
| Herchy | Mooney viscosity | Mooney viscosity | Mooney viscosity | Ethylene maʻiʻo | Maʻiʻo propylene | ʻIke ENB | Hoʻonui-ʻaila maʻiʻo | Palapala noi | ʻAno |
| Papa |
ML(1+4)100 ℃ | ML(1+4)125 ℃ | ML(1+4)150 ℃ | wt% | wt% | wt% | PHR | ||
| CO 033 | 30 | 72 | 28 | ||||||
| CO 034 | 44 | 72 | 28 | ||||||
| CO 038 | 60 | 72 | 28 | ||||||
| CO 043 | 33 | 55 | 45 | ||||||
| CO 054 | 44 | 59 | 41 | ||||||
| CO 058 | 80 | 60 | 52 | 48 | |||||
| CO 059 | 79 | 59 | 41 | ||||||
| TER 4033 | 30 | 70 | 25 | 5 | ʻO nā huahana paʻakikī kiʻekiʻe; Nā Huahana Hoʻoheheʻe Hoʻoheheʻe ʻia; ʻO ke sila ʻili kaʻa kaʻa | Haʻahaʻa Mooney viscosity; ʻO ka wai maikaʻi; ʻO ka nui o ka ethylene; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi |
|||
| TER 4038EP | 60 | 68.6 | 27 | 4.4 | Hose; Nā ʻāpana hoʻopaʻa puka a me ka puka makani; Huahana Extrusion; | ʻO ka nui o ka ethylene; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi |
|||
| TER 4039 | 77 | 68.6 | 27 | 4.4 | Hose; Nā ʻāpana hoʻopaʻa puka a me ka puka makani; Huahana Extrusion; | ʻO ka nui o ka ethylene; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi |
|||
| TER 4044 | 44 | 61 | 35 | 4 | ʻO nā huahana hoʻoheheʻe ʻia; | Haʻahaʻa Mooney viscosity; ʻO ka wai maikaʻi; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi |
|||
| TER 4047 | 55 | 55.5 | 40 | 4.5 | Hose Paʻa; Nā huahana i hoʻoheheʻe ʻia; Gasket; Nā ʻāpana mīkini hana; | Haʻahaʻa ethylene maʻiʻo; Ka waiwai hana maikaʻi; Kūleʻa wela haʻahaʻa |
|||
| TER 4049 | 76 | 55.5 | 40 | 4.5 | Hose; Hoʻopaʻa paʻa paʻa; Gasket; Nā huahana ʻoihana; | Haʻahaʻa ethylene maʻiʻo; Nā waiwai mechanical kiʻekiʻe; Kūleʻa wela haʻahaʻa |
|||
| TER 4334 | 28 | 68.3 | 27 | 4.7 | 43 | ʻO nā huahana paʻakikī kiʻekiʻe; Nā huahana hoʻoheheʻe injection; Nā mea hoʻopaʻa paʻa kaʻa kaʻa; Nā huahana ʻoihana | Haʻahaʻa Mooney viscosity; ʻO ka wai maikaʻi; ʻO ka nui o ka ethylene; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi |
||
| TER 4436 | 43 | 66.5 | 28 | 5.5 | 67 | ʻO nā sila puka mīkini holoi; Nā huahana ʻoihana | Ka waiwai hana maikaʻi; Nā waiwai mechanical kiʻekiʻe; |
||
| TER 4437 | 57 | 63.5 | 32 | 4.5 | 67 | ʻO nā sila puka mīkini holoi; | Ka waiwai hana maikaʻi; Nā waiwai mechanical kiʻekiʻe; Kūleʻa wela kiʻekiʻe; |
||
| TER 4535 | 32 | 64.6 | 32 | 3.4 | 100 | ʻO nā sila puka mīkini holoi; | Haʻahaʻa ENB maʻiʻo; Kūleʻa wela kiʻekiʻe; |
||
| TER 6148 | 65 | 53 | 40 | 7 | 18 | Nā ʻāpana i hoʻoheheʻe ʻia; Hōʻikeʻike sponge; Nā huahana i hoʻoheheʻe ʻia; | Haʻahaʻa ethylene maʻiʻo; Maikaʻi ENB kiʻekiʻe; wikiwiki ho'ōla wikiwiki; Kūleʻa wela haʻahaʻa |
||
| TER 6235 | 33 | 60.6 | 32 | 7.4 | 30 | ʻO loko o loko; Kāmaʻa; Nā ʻāpana i hoʻoheheʻe ʻia; Hōʻikeʻike sponge; Nā huahana i hoʻoheheʻe ʻia | Haʻahaʻa Mooney viscosity; ʻO ka wai maikaʻi; ʻO ka nui o ka ethylene; Nā waiwai mechanical kiʻekiʻe; Ka waiwai hana maikaʻi; Maikaʻi ENB kiʻekiʻe; wikiwiki ho'ōla wikiwiki; |
||
| TER 6537 | 43 | 60 | 32 | 8 | 100 | ʻO nā ʻāpana i hoʻoheheʻe ʻia; Hōʻikeʻike sponge; ʻO nā sila puka mīkini holoi; Nā huahana i hoʻoheheʻe ʻia | Maikaʻi ENB kiʻekiʻe; wikiwiki ho'ōla wikiwiki; |
||
| TER 9046 | 67 | 60.1 | 31 | 8.9 | ʻO nā ʻāpana i hoʻoulu ʻia; Hōʻikeʻike sponge; Nā huahana ʻoihana | Maikaʻi ENB kiʻekiʻe; wikiwiki ho'ōla wikiwiki; |
|||
| TER 4548 | 47 | 59.5 | 36 | 4.5 | 10 | ʻO loko o loko; Kāma; Nā huahana i hoʻoheheʻe ʻia ; Nā huahana ʻoihana; Nā huahana i hoʻoheheʻe ʻia | Haʻahaʻa Mooney viscosity; ʻO ka wai maikaʻi; |
||
| TER 8148 | 68 | 52.5 | 39 | 8.5 | 21 | Nā ʻāpana hoʻoheheʻe ʻia; Hōʻikeʻike sponge; Nā huahana ʻoihana; Nā huahana i hoʻoheheʻe ʻia | Haʻahaʻa ethylene maʻiʻo; Maikaʻi ENB kiʻekiʻe; wikiwiki ho'ōla wikiwiki; Kūleʻa wela haʻahaʻa |
||
| TER 7040 | 87 | 53.5 | 40 | 6.5 | Hose; Nā ʻāpana hoʻopaʻa puka a me ka puka makani; Huahana Extrusion; | Haʻahaʻa ethylene maʻiʻo; Hoʻopiha kiʻekiʻe; Kiʻekiʻe Mooney viscosity; Nā waiwai mechanical kiʻekiʻe; Kūleʻa wela haʻahaʻa |
|||
| TER 4049 | 76 | 55.5 | 40 | 4.5 | Hose; Nā ʻāpana hoʻopaʻa puka a me ka puka makani; Huahana Extrusion; | Haʻahaʻa ethylene maʻiʻo; Kūleʻa wela haʻahaʻa |
|||
| TER 5029 | 80 | 69.5 | 25 | 5.5 | Hose; Nā ʻāpana hoʻopaʻa puka a me ka puka makani; Huahana Extrusion; | Hoʻopiha kiʻekiʻe; ʻO ka nui o ka ethylene; Kiʻekiʻe Mooney viscosity; Nā waiwai mechanical kiʻekiʻe |
1. Kaʻa hoʻopaʻa kaula
ʻAi hoʻopaʻa no ka puʻupuʻu
Sila puka
Palena pukaaniani
ʻO ka hoʻopaʻa ʻana o ka sunroof
Sila kaʻa
Anti-puehu
Kaila Glassrun
Kūleʻa-leo
2. Hose
Nā paipu kaʻa
Hose radiator kaʻa
Paipu hoʻoheheʻe Skylight
3. Uea a me ke kaula
Uea mana
Uea i uhi ʻia i ka Rubber
uwea kūloko
Uea televise
Uea mea kani
4. Puka wai
ʻO ka wili wai pā
ʻO ka wili wai o ka hale
ʻO ka ʻōwili wai ala alanui
Tunnel wili wai
5. Na huila
Pupu loko
ʻaoʻao pāka
Paa paikikala
6. Nā huahana hoʻoheheʻe maʻamau
Palapa lāʻau
Moena lāʻau
Hoʻopaʻa
Pāʻani kīʻaha
7. Hoʻololi aila a me nā māla ʻē aʻe
lubricant mea hoʻohui