FV9600 Fluorosilicone

Loaʻa i kēia huahana ka pale ahi maikaʻi, e hālāwai me UL94/FV 0 pae pale ahi. ʻOi aku ka maikaʻi o ke kūpaʻa aila, ka pale ʻana i ka solvent, ka pale wela kiʻekiʻe a me ka haʻahaʻa
  • FV9600

  • Herchy

Loaʻa:
Nui:

Nā hōʻailona ʻenehana

Nā mea

Papa kuhikuhi

Papa

FV9660

FV9670

Ka nana aku

Nā ʻano hoʻāʻo

Keʻokeʻo

Kaumaha kikoʻī/g/cm3

ASTM D792

1.46

1.48

Paʻakikī/kahakaiA

ASTM D2240

60

70

Ikaika U'i/MPa

ASTM D412

6.8

6.5

Elongation ma ka hoomaha /%

ASTM D412

310

290

Ka Haehae Kaha/KN/m

ASTM D624-B

17

17

*Papa wela
200 ℃×72h

Hoʻololi paʻakikī / kahakai A

+5

+5

Hoʻololi ikaika tensile, %

3.8

3.5

Hoʻololi ikaika tensile, %

161

154

IRM903
Hoʻololi Volume/%
150 ℃/72h

ASTM D471

5.5

5.2

Huina C
Ka nui o ka hoololi/%
23℃/72h

ASTM D471

20

20

Papa-pale ahi

GBT10707-2008

FV 0

FV 0

Kūlana hoʻōla

Hoʻohui i 0.7 mau ʻāpana o ka bis(2+5), hoʻokahi pae vulcanization 170 ℃ × 15min, ʻelua pae vulcanization: 200 ℃ × 4h.


Nā ʻōlelo paipai


e hoʻohana i ka 0.6 a i ka 1 ʻāpana bis-dipenta vulcanising agent(2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).

Hoʻoholo ʻia ka mahana mālama a me ka manawa e like me ka nui o ka huahana a me ke ʻano o ka mālama ʻana i hana ʻia e ka mea kūʻai.

Hoʻopaʻa Huahana ʻO


kēia huahana he waiwai ʻAʻole pilikia, pahu pahu pahu, ʻeke ʻeke ʻeke i loko, ʻumi kilokani no ka ʻeke, ʻelua ʻeke no ka pahu.

Ka wā mālama


No ka loaʻa ʻana o nā waiwai kahe o kēia huahana, i ka wā o ka lawe ʻana a me ka hoʻohana ʻana, pono e pale ʻia ka ʻeke e haki.

E mālama i loko o kahi maloʻo maloʻo no 12 mahina.

Mua: 
Aʻe: 

NUI WIWIKI

KO MAKOU HANA

IKE HOPE

Hoʻohui: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
leka uila:  info@herchyrubber.com
Kuleana kope     2023 Shanghai Herchy Rubber Co., Ltd. Palapala kahua |   Kulekele pilikino | Kākoʻo Na Leadong.