Hydrogenated nitrile rubber precompound a me ka hui-HNBR
Hydrogenated nitrile rubber (HNBR a i ʻole HSN) ka huahana o ka hydrogenation a me ka saturation o ka carbon-carbon paʻa pālua i loko o ke kaulahao mole o ka nitrile rubber, no laila ua kapa ʻia ʻo ia no ka nitrile rubber saturated.
Hiki i ka HNBR ke kū'ē i kaʻaila maikaʻi (kū'ē maikaʻi i kaʻaila hinu, lubricants, aromatic solvents); a ma muli o kona ʻano hoʻoheheʻe nui ʻia, maikaʻi ke kūpaʻa wela, ke kūpaʻa maikaʻi maikaʻi (kū kūʻē maikaʻi iā Freon, nā waikawa a me nā alkalis), ke kūpaʻa ozone maikaʻi, a me ke kūpaʻa kiʻekiʻe i ka deformation mau loa i ka hoʻoemi; i ka manawa like, loaʻa iā HNBR ka ikaika kiʻekiʻe, ka hana haehae kiʻekiʻe. Loaʻa i ka HNBR ka ikaika kiʻekiʻe, ka hana waimaka kiʻekiʻe, ke kūpaʻa maikaʻi o ka lole, a me nā mea ʻē aʻe.
He hui ʻenehana loea ʻo Herchy Rubber me ka ʻike waiwai ma HNBR R&D. Hiki iā mākou ke hoʻomohala i nā huahana no nā noi like ʻole e like me nā pono o nā mea kūʻai aku. A hauʻoli i ka inoa kiʻekiʻe ma Kina a me ka honua.
| Herchy | ʻAno vulcanization | ʻO ka maʻiʻo Acrylonitrile | Mooney viscosity | ʻoʻoleʻa | Ka ikaika tensile | Elongation i ka wā hoʻomaha | IRM 903 Hoʻololi leo | Hoʻonohonoho hoʻoemi | Palapala noi | ʻAno |
| 150℃*72h | 150 ℃*72h ASTM D395 ʻAno B | |||||||||
| Papa | % | ML(1+4)100 ℃ | Kahakai A | Mpa | % | % | % | |||
| HNBR-S6035 | Sulfur | 35 | 50~100 | 60 | 17~24 | 300~500 | <20 | <60 | Nā huahana i ka ʻoihana ʻaila hinu, | ʻO ka elongation nui, Hoʻopili ponoʻī maikaʻi, hana maikaʻi loa |
| HNBR-S7035 | Sulfur | 35 | 50~100 | 70 | 17~24 | 300~500 | <20 | <60 | Nā huahana ma ka ʻoihana ʻaila, ʻoihana kaʻa, Belt |
ʻO ke kūpaʻa luhi ikaika , Kūʻai kūʻokoʻa maikaʻi, ka hana maikaʻi loa |
| HNBR-S8035 | Sulfur | 35 | 50~100 | 80 | 17~24 | 300~500 | <20 | <60 | ʻO nā papa pale pale wili, Ppressure accumulators |
Kiʻekiʻe puʻe kū'ē, Good self-adhesiveness |
| HNBR-S6043 | Sulfur | 43 | 50~100 | 60 | 17~24 | 300~500 | <10 | <60 | Wahi kaʻa, Nā huahana ma ka ʻoihana ʻaila |
ʻAila pale, Exllent hana |
| HNBR-S7043 | Sulfur | 43 | 50~100 | 70 | 17~24 | 300~500 | <10 | <60 | Nā huahana ma ka ʻoihana ʻaila, ʻoihana kaʻa, |
ʻAila kūʻē, Dynamic fatigue resistance , Kūʻē ponoʻī maikaʻi |
| HNBR-S8043 | Sulfur | 43 | 50~100 | 80 | 17~24 | 300~500 | <10 | <60 | ʻO nā papa pale pale wili, Ppressure accumulators |
ʻO kaʻaila pale, High pressure resistance, Good self-adhesiveness |
| HNBR-P6035 | Peroxide | 35 | 50~100 | 60 | 17~24 | 200~350 | <20 | <30 | ʻOihana kaʻa, ʻoihana hana mokulele |
Kiʻekiʻe tempreture kū'ē, Exllent hana |
| HNBR-P7035 | Peroxide | 35 | 50~100 | 70 | 17~24 | 200~350 | <20 | <30 | ʻOihana hana, ʻenekini gaskets, O-rings, Sila |
Kiʻekiʻe tempreture kū'ē, maikaʻi hoʻopaʻa 'ia |
| HNBR-P8035 | Peroxide | 35 | 50~100 | 80 | 17~24 | 200~350 | <20 | <30 | Nā paipu wili, nā mea hoʻoemi kaomi, |
Ke kū'ē kū'ē ki'eki'e, High tempreture resistance |
| HNBR-P6043 | Peroxide | 43 | 50~100 | 60 | 17~24 | 200~350 | <10 | <30 | Huina kaʻa a me nā ʻōnaehana Lubrication | ʻO ke kūpaʻa ʻaila, ka hana maikaʻi loa, ka hoʻonohonoho hoʻopili maikaʻi |
| HNBR-P7043 | Peroxide | 43 | 50~100 | 70 | 17~24 | 200~350 | <10 | <30 | ʻO nā ʻenekini, nā apo-O, nā Sila, Belt |
ʻO ke kūpaʻa ʻaila, ka hoʻonohonoho hoʻoemi maikaʻi, ka hana maikaʻi loa |
| HNBR-P8043 | Peroxide | 43 | 50~100 | 80 | 17~24 | 200~350 | <10 | <30 | Nā paipu wili, Nā mea hoʻoemi kaomi |
ʻO kaʻaila pale, High pressure resistance, High tempreture resistance |
1. kāʻei Triangular
2. Nā mea hoʻokaʻawale haʻalulu
3.
Sila
4. Paipu pale wela
5.
Pahu pale wili
6. Pistons no ka paila lepo
7.
ʻO ka hoʻopaʻa ʻana i nā gaskets no ka ʻoihana kaʻa
8. Sila no na hale mana
9.
Nā paipu wai hydraulic
10. Na sila hydraulic
11. Na kaula uwea no na hale mana
12. Pa'i a me ka lole wili
13. Sila no ka aerospace
14. Uhi
15.Fuel pūpū