FV9500
Herchy
| Loaʻa: | |
|---|---|
| Nui: | |
Nā hōʻailona ʻenehana
Nā mea |
Nā hōʻailona |
||||
Papa |
FV9540 |
FV9550 |
FV9560 |
FV9561 |
|
Ka nana aku Nā ʻano hoʻāʻo |
melemele |
||||
Kaumaha kikoʻī/ g/cm3 |
ASTM D792 |
1.40 |
1.41 |
1.42 |
1.44 |
Paʻakikī/kahakaiA |
ASTM D2240 |
41 |
50 |
60 |
61 |
Ikaika U'i/MPa |
ASTM D412 |
9.5 |
9.8 |
10.2 |
9.8 |
Elongation ma ka hoomaha /% |
ASTM D412 |
370 |
282 |
263 |
310 |
Ka Haehae Kaha/KN/m |
ASTM D624-B |
17 |
17 |
18 |
17 |
*Ke kū'ē wela |
Hoʻololi paʻakikī / kahakai A |
+4 |
+2 |
+2 |
+2 |
Hoʻololi ikaika tensile, % |
-24 |
-25 |
-23 |
-26 |
|
Elongation i ka hoʻololi hoʻomaha, % |
-19 |
-10 |
-14 |
-12 |
|
Huina C Hoʻololi Volume/% 23℃/72h |
ASTM D471 |
+23 |
+23 |
+21 |
+21 |
Peel Strength/N/mm, me Methyl vinyl silicone rubber |
2.0 |
2.0 |
2.2 |
2.0 |
|
Kūlana hoʻōla |
E hoʻohui i 0.8 mau ʻāpana o ka bis-di-quaternary, hoʻokahi pae vulcanization 120 ℃ × 15min, ʻelua pae vulcanization: 200 ℃ × 4h |
||||
Kū'ē Kiʻekiʻe i nā Kaiapuni Koʻikoʻi : FV9500 fluorosilicone rubber ʻoi aku ka maikaʻi i nā kaiapuni me nā wela wela a me ka ʻike ʻana i nā kemika hoʻopaʻapaʻa. Hāʻawi ia i ke kūpaʻa maikaʻi loa i nā wahie, nā aila, a me kahi ākea o nā kemika, e kūpono ana no ka koi ʻana i nā noi ʻoihana.
Laulā Wehewela Laulā : Hāʻawi kēia mea i kahi ākea ākea ākea, mai ka haʻahaʻa -60 ° C a hiki i ka 200 ° C. ʻO kēia ka mea kūpono loa no nā noi i nā ʻoihana automotive, aerospace, a me nā ʻoihana hana, kahi e maʻamau ai ka fluctuations o ka mahana.
ʻOi aku ka maikaʻi o ka hoʻopaʻa ʻana i ka hoʻopaʻa ʻana : FV9500 e hōʻike ana i ke kūʻē kūʻokoʻa i ka hoʻonohonoho hoʻopili, e hōʻoia ana i ka hana lōʻihi a me ka hoʻopaʻa ʻana i ka pono ma lalo o ke kaomi hoʻomau, ʻoiai i nā kūlana koʻikoʻi.
Hoʻonui i ka Durability : Hoʻonui ka hui fluorosilicone i ka lōʻihi e kū'ē i kaʻelemakule, ka ozone, a me ka hōʻike UV, e hōʻoia ana i ka hilinaʻi lōʻihi a me ka hana, ʻoiai ma lalo o nā kūlana kūlohelohe.
ʻO ka Insulation Electrical Superior : Hāʻawi ia i nā waiwai insulation uila maikaʻi loa, kūpono ia no ka hoʻohana ʻana i nā ʻāpana uila a me nā noi hoʻopaʻa ʻana i kahi mea koʻikoʻi ke kūpaʻa uila.
Versatility in Application : Hiki ke hoʻohana ʻia ka mea ma waena o nā ʻoihana like ʻole, me ka automotive, aerospace, aila a me ke kinoea, a me nā mea uila, ma muli o kona hui pū ʻana o ka ikaika mechanical a me ke kūpaʻa kemika.
Hoʻololi maikaʻi a me ka pale ʻana i ka waimaka : Hāʻawi ʻo Fluorosilicone rubber FV9500 i ka hiki ke hiki i nā haʻahaʻa haʻahaʻa, i hui pū ʻia me ka waimaka maikaʻi a me ke kūpaʻa abrasion, e hōʻoiaʻiʻo ana i ka hana hilinaʻi i nā kūlana dynamic a kiʻekiʻe.
Loaʻa nā koho meaʻai : Ma muli o kāu mau koi, hiki ke hoʻokumu ʻia nā ʻano ʻano fluorosilicone rubber no ka hoʻokō ʻana i nā kūlana meaʻai, e hāʻawi ana i kahi hopena palekana no nā noi i ka hana meaʻai a me nā ʻoihana lāʻau.