FV9700 Fluorosilicone

He kūpono kēia huahana no ka hoʻoheheʻe ʻana i ka bis-disulfide. Loaʻa iā ia ke kūpaʻa aila maikaʻi, ka pale ʻana i ka solvent, ka waikawa a me ke kūpaʻa alkali.
  • FV9700

  • Herchy

Loaʻa:
Nui:

Nā hōʻailona ʻenehana



'ikamu

Nā hōʻailona

Helu

NFS9760

NFS9770

Ka nana aku

Nā ʻano hoʻāʻo

ʻili ʻulaʻula, ʻoluʻolu,

ʻAʻohe haumia

Kaumaha kikoʻī/ g/cm3

ASTM D792

1.44

1.48

Paʻakikī/kahakaiA

ASTM D2240

60

70

Ikaika U'i/MPa

ASTM D412

10.5

10.1

Elongation ma ka hoomaha /%

ASTM D412

207

201

Ka Haehae Kaha/KN/m

ASTM D624-B

18

17

Hoʻonohonoho hoʻoemi (177 ℃*22h)

Hoʻololi paʻakikī/A

+4

+5

Ka nui o ka hoʻololi o ka ikaika tensile/%

-27

-24

Ka helu o ka hoʻololi o ka elongation/%

-26

-23

Huina C

Hoʻololi Volume/%

23℃/72h

ASTM D471

21

20

IRM903
Ka nui o ka hoʻololi ʻana/%
150℃×72h

ASTM D471

4.5

4

ʻAka Nitric/ʻakika sulfuric/ʻakika hydrochloric i hui pū ʻia ka hopena PH<1 100℃×120h

ʻO ke kūpaʻa ʻana i ka ʻakika
.

ASTM D471

0.3

0.3

3% solution sodium hydroxide 60 ℃×72h

ʻO ke kūpaʻa alkaline
ka nui o ka hoʻololi ʻana o ka nui/%

ASTM D471

0.4

0.3

Kūlana hoʻōla

0.8 mau ʻāpana o ka bisditetra, hoʻokahi pae vulcanization 120 ℃ × 15min, ʻelua-pae vulcanization: 200 ℃ × 4h

Nā hana i paipai ʻia:


Manaʻo ʻia e hoʻohana i nā ʻāpana 0.4-0.7 o bisdisulfide (2,5-dimethyl-2,5-bis(tert-butylperoxy) hexane).


Pono nā mea kūʻai e koho i ka mahana a me ka manawa kūpono no ka ho'ōla ʻana ma muli o ka nui o ka huahana a me ke ʻano o ka ho'ōla ʻana.


Puke huahana:


ʻAʻole pōʻino kēia huahana, ua haku ʻia me ka pahu pahu, plastik, a me 10 kilokani no ka ʻeke, 2 ʻeke no ka pahu.


Makahiki o ka waiho ʻana:


Hiki i kēia huahana ke kahe anuanu, pono e pale ʻia ka ʻeke i ʻole e pōʻino i ka wā o ka lawe ʻana a i ʻole ka hoʻohana ʻana.


E mālama i loko o kahi wahi maloʻo maloʻo me 12 mahina.


Mua: 
Aʻe: 

NUI WIWIKI

KO MAKOU HANA

IKE HOPE

Hoʻohui: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Kuleana kope     2023 Shanghai Herchy Rubber Co., Ltd. Palapala kahua |   Kulekele pilikino | Kākoʻo Na Leadong.