GA-96XX
Herchy
| Argaeledd: | |
|---|---|
| Nifer: | |
Cais: addas ar gyfer cynhyrchu gwres dargludol tâp rwber silicon, gasged dargludol thermol ac ati.
Nodweddion allweddol: cryfder uchel, gall dargludedd thermol gyrraedd 0.5 -2w / mxk, pasio dilysiad RoHS a REACH.
Prawf: 1% o asiant halltu (50% past o DBPMH mewn silicongum), 175 ℃ x5 munud x 15MPa.
| Paramedrau cynnyrch | ||||||||
| Cynnyrch | GA-9630 | GA-9640 | GA-9650 | GA-9660 | GA-9670 | GA-9680 | GA-9680B | |
| Ymddangosiad | Llwyd | Du | ||||||
| William plastigrwydd | 160 | 180 | 200 | 220 | 240 | 270 | 270 | |
| Caledwch (ShoreA) | 30 | 40 | 50 | 60 | 70 | 76 | 79 | |
| Dwysedd(g/cm3) | 2.1 | 2.13 | 2.15 | 2.2 | 2.25 | 2.04 | 2.35 | |
| Cryfder tynnol (MPa) | 1 | 1.5 | 2 | 2 | 2.5 | 4.5 | 4.7 | |
| elongation(%) | 800 | 750 | 700 | 600 | 500 | 80 | 130 | |
| Cryfder dagrau (kN/m) | 6 | 6 | 6 | 10 | 10 | 8 | 11.3 | |
| Cyfernod dargludedd thermol (W / MK) | 0.8 | 0.8 | 0.8 | 0.9 | 0.9 | 0.8 | 0.9 | |