GA-96XX
Herchy
| Avanoa: | |
|---|---|
| Aofa'i: | |
Talosaga: talafeagai mo le gaosiga o le vevela conductive silicone pa'u lipine, vevela conductive gasket ma isi.
Autu autu: malosi maualuga, faʻauluina vevela e mafai ona oʻo atu i le 0.5 -2w / mxk, pasi le faʻamaoniga o le RoHS ma le REACH.
Su'ega: 1% o le fa'amalolo fa'amalolo (50% pa'u o le DBPMH i le siliconegum), 175 ℃ x5min x 15MPa.
| Fa'atauga o oloa | ||||||||
| Oloa | GA-9630 | GA-9640 | GA-9650 | GA-9660 | GA-9670 | GA-9680 | GA-9680B | |
| Fa'aaliga | Lanu efuefu | Lanu uliuli | ||||||
| William palasiti | 160 | 180 | 200 | 220 | 240 | 270 | 270 | |
| Malosi (ShoreA) | 30 | 40 | 50 | 60 | 70 | 76 | 79 | |
| Malosi (g/cm3) | 2.1 | 2.13 | 2.15 | 2.2 | 2.25 | 2.04 | 2.35 | |
| Malosi fa'amalosi (MPa) | 1 | 1.5 | 2 | 2 | 2.5 | 4.5 | 4.7 | |
| Fa'atele(%) | 800 | 750 | 700 | 600 | 500 | 80 | 130 | |
| Malosi o loimata (kN/m) | 6 | 6 | 6 | 10 | 10 | 8 | 11.3 | |
| Coefficient of conductivity vevela(W/MK) | 0.8 | 0.8 | 0.8 | 0.9 | 0.9 | 0.8 | 0.9 | |