ꯖꯤ.ꯑꯦ.-꯹꯶ꯑꯦꯛꯁ.ꯑꯦꯛꯁ
ꯍꯔꯆ꯭ꯆꯤ ꯑꯣꯏꯕꯥ ꯌꯥꯏ꯫
| ꯐꯪꯒꯗꯕꯥ: | |
|---|---|
| ꯃꯁꯤꯡ: ꯱. | |
ꯑꯦꯞꯂꯤꯀꯦꯁꯟ: ꯍꯤꯠ ꯀꯟꯗꯨꯛꯇꯤꯚ ꯁꯤꯂꯤꯀꯣꯟ ꯔꯕ꯭ꯕꯔ ꯇꯦꯞ, ꯊꯔꯃꯦꯜ ꯀꯟꯗꯨꯛꯇꯤꯚ ꯒ꯭ꯌꯥꯁꯀꯦꯠ ꯑꯁꯤꯅꯆꯤꯡꯕꯥ ꯄꯨꯊꯣꯀꯄꯗꯥ ꯆꯨꯅꯕꯥ꯫
ꯃꯔꯨꯑꯣꯏꯕꯥ ꯃꯁꯀꯁꯤꯡ: ꯑꯋꯥꯡꯕꯥ ꯁꯛꯇꯤ, ꯊꯔꯃꯦꯜ ꯀꯟꯗꯨꯛꯇꯤꯕꯤꯇꯤꯅꯥ ꯰.꯵ -꯲w/mxk ꯌꯧꯕꯥ ꯉꯝꯃꯤ, RoHS ꯑꯃꯁꯨꯡ REACHꯒꯤ ꯑꯣꯊꯦꯟꯇꯤꯀꯦꯁꯟ ꯄꯥꯁ ꯇꯧꯕꯥ ꯉꯝꯃꯤ꯫
ꯇꯦꯁ꯭ꯠ: ꯀ꯭ꯌꯨꯔꯤꯡ ꯑꯦꯖꯦꯟꯇꯀꯤ 1% (ꯁꯤꯂꯤꯀꯣꯅꯦꯒꯃꯗꯥ DBPMHꯒꯤ ꯄꯦꯁ꯭ꯠ 50%), 175°Cx5min x 15MPa꯫
| ꯄ꯭ꯔꯗꯛꯇ ꯄꯦꯔꯥꯃꯤꯇꯔꯁꯤꯡ꯫ | ||||||||
| ꯄꯣꯠꯊꯣꯛ | ꯖꯤ.ꯑꯦ.-꯹꯶꯳꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯶꯴꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯶꯵꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯶꯶꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯶꯷꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯶꯸꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯶꯸꯰ꯕꯤ | |
| ꯃꯄꯥꯟꯊꯣꯡꯗ ꯎꯕ | ꯁꯃꯨ ꯝꯆꯨ | ꯑꯃꯨꯕ | ||||||
| ꯎꯏꯂꯤꯌꯥꯝ ꯄ꯭ꯂꯥꯁ꯭ꯇꯤꯁꯤꯇꯤ꯫ | 160 | 180 | 200 | 220 | 240 | 270 | 270 | |
| ꯍꯥꯔꯗꯅꯦꯁ (ꯁꯣꯔꯑꯦ) ꯑꯃꯁꯨꯡ ꯑꯦꯟ. | 30 | 40 | 50 | 60 | 70 | 76 | 79 | |
| ꯗꯦꯟꯁꯤꯇꯤ(ꯖꯤ/ꯁꯦ.ꯃꯤ.꯳) ꯑꯁꯤꯅꯤ꯫ | 2.1 | 2.13 | 2.15 | 2.2 | 2.25 | 2.04 | 2.35 | |
| ꯇꯦꯟꯁꯥꯏꯜ ꯁ꯭ꯠꯔꯦꯡꯊ (ꯑꯦꯝ.ꯄꯤ.ꯑꯦ.) ꯑꯁꯤ ꯌꯥꯑꯣꯔꯤ꯫ | 1 | 1.5 | 2 | 2 | 2.5 | 4.5 | 4.7 | |
| ꯏꯂꯣꯡ ꯇꯧꯕꯥ(%) | 800 | 750 | 700 | 600 | 500 | 80 | 130 | |
| ꯇꯤꯌꯥꯔ ꯁ꯭ꯠꯔꯦꯡꯊ (ꯀꯦ.ꯑꯦꯟ./ꯑꯦꯝ.) | 6 | 6 | 6 | 10 | 10 | 8 | 11.3 | |
| ꯊꯔꯃꯦꯜ ꯀꯟꯗꯨꯛꯇꯤꯕꯤꯇꯤꯒꯤ ꯀꯣꯑꯣꯐꯤꯁꯤꯑꯦꯟꯁꯤ(ꯗꯕꯜꯌꯨ/ꯑꯦꯝ.ꯀꯦ.) | 0.8 | 0.8 | 0.8 | 0.9 | 0.9 | 0.8 | 0.9 | |