Dɔwɔwɔ: sɔ na dzoxɔxɔ si kplɔa silicone rababa tape, dzoxɔxɔ kplɔa gasket kple bubuawo wɔwɔ.
Nu veviwo: ŋusẽ gã, dzoxɔxɔ ƒe tsɔtsɔme ate ŋu aɖo 0.5 -2w/mxk, ato theauthentication ƒe RoHS kple REACH.
Dodokpɔ: 1% le atike si daa gbe le ame ŋu (50% ƒe atike si wotsɔ DBPMH wɔe le siliconegum me), 175°Cx5min x 15MPa.
| Nusiwo wowɔ ƒe nɔnɔmewo | ||||||||
| Nu si wowɔ | GA-9630 ƒe agbalẽa | GA-9640 ƒe agbalẽa | GA-9650 ƒe agbalẽa | GA-9660 ƒe agbalẽa | GA-9670 ƒe agbalẽa | GA-9680 ƒe agbalẽa | GA-9680B ƒe agbalẽa | |
| Dzedzeme | Fu | Yibᴐ | ||||||
| William ƒe plasticity | 160 | 180 | 200 | 220 | 240 | 270 | 270 | |
| Sesẽme (ƑutaA) . | 30 | 40 | 50 | 60 | 70 | 76 | 79 | |
| Eƒe kpekpeme(g/cm3) . | 2.1 | 2.13 | 2.15 | 2.2 | 2.25 | 2.04 | 2.35 | |
| Ŋusẽ si wotsɔna ƒoa nu (MPa) . | 1 | 1.5 | 2 | 2 | 2.5 | 4.5 | 4.7 | |
| Elongation(%) ƒe didime . | 800 | 750 | 700 | 600 | 500 | 80 | 130 | |
| Aɖatsi ƒe ŋusẽ (kN/m) . | 6 | 6 | 6 | 10 | 10 | 8 | 11.3 | |
| Dzoxɔxɔ ƒe tsɔtsɔme ƒe xexlẽdzesi(W/MK) . | 0.8 | 0.8 | 0.8 | 0.9 | 0.9 | 0.8 | 0.9 | |