GA-96XX
Herchy
| kupezeka: | |
|---|---|
| kuchuluka: | |
Ntchito: oyenera kupanga kutentha conductive silikoni mphira tepi, matenthedwe conductive gasket ndi zina zotero.
Zofunikira zazikulu: mphamvu yayikulu, matenthedwe amatenthedwe amatha kufikira 0.5 -2w/mxk, kudutsa kutsimikizika kwa RoHS ndi REACH.
Mayeso: 1% ya machiritso (50% phala la DBPMH mu siliconegum), 175 ℃x5min x 15MPa.
| Mankhwala magawo | ||||||||
| Zogulitsa | GA-9630 | GA-9640 | GA-9650 | GA-9660 | GA-9670 | GA-9680 | GA-9680B | |
| Maonekedwe | Imvi | Wakuda | ||||||
| William plasticity | 160 | 180 | 200 | 220 | 240 | 270 | 270 | |
| Kuuma (ShoreA) | 30 | 40 | 50 | 60 | 70 | 76 | 79 | |
| Kachulukidwe (g/cm3) | 2.1 | 2.13 | 2.15 | 2.2 | 2.25 | 2.04 | 2.35 | |
| Mphamvu yamagetsi (MPa) | 1 | 1.5 | 2 | 2 | 2.5 | 4.5 | 4.7 | |
| Kutalikira (%) | 800 | 750 | 700 | 600 | 500 | 80 | 130 | |
| Mphamvu yamisozi (kN/m) | 6 | 6 | 6 | 10 | 10 | 8 | 11.3 | |
| Coefficient of thermal conductivity (W/MK) | 0.8 | 0.8 | 0.8 | 0.9 | 0.9 | 0.8 | 0.9 | |