GA-96XX Thermal Conductive Silicone Rubber (HCR)

GA-96XX Thermal conductive silicone rubber (HCR)
Kushandisa: kwakakodzera kugadzirwa kwekupisa conductive silicone rubber tepi, thermal conductive gasket uye zvichingodaro.
Akakosha maficha: yakakwira simba, yekupisa conductivity inogona kusvika 0.5 -2w/mxk, pfuura kusimbiswa kweRoHS uye REACH.
  • GA-96XX

  • Herchy

Kuwanikwa:
Huwandu:
GA-96XX Thermal conductive silicone rubber (HCR)


Kushandisa: kwakakodzera kugadzirwa kwekupisa conductive silicone rubber tepi, thermal conductive gasket uye zvichingodaro.
Akakosha maficha: yakakwira simba, yekupisa conductivity inogona kusvika 0.5 -2w/mxk, pfuura kusimbiswa kweRoHS uye REACH.
Muedzo: 1% yekurapa mumiririri (50% paste yeDBPMH musiliconegum), 175 ℃ x5min x 15MPa.


Product parameters




Product GA-9630 GA-9640 GA-9650 GA-9660 GA-9670 GA-9680 GA-9680B
Chitarisiko Gireyi

Nhema

William plastiki 160 180 200 220 240 270 270
Kuoma (ShoreA) 30 40 50 60 70 76 79
Density(g/cm3) 2.1 2.13 2.15 2.2 2.25 2.04 2.35
Tensile simba (MPa) 1 1.5 2 2 2.5 4.5 4.7
Elongation(%) 800 750 700 600 500 80 130
Simba rekubvarura (kN/m) 6 6 6 10 10 8 11.3
Coefficient of thermal conductivity (W/MK) 0.8 0.8 0.8 0.9 0.9 0.8 0.9


Zvakapfuura: 
Zvinotevera: 

KUKURUMIDZA ZVINONYANYA

ZVINHU ZEDU

CONTACT INFORMATION

Wedzera: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.