GA-96XX
Herchy
| Kasadiaan: | |
|---|---|
| Kuantitas: | |
Aplikasi: cocog pikeun produksi panas conductive tape karét silicone, gasket conductive termal jeung saterusna.
Fitur konci: kakuatan tinggi, konduktivitas termal tiasa ngahontal 0.5 -2w / mxk, lulus auténtikasi RoHS sareng REACH.
Uji: 1% tina agén curing (50% némpelkeun DBPMH dina siliconegum), 175 ℃ x5min x 15MPa.
| Parameter produk | ||||||||
| produk | GA-9630 | GA-9640 | GA-9650 | GA-9660 | GA-9670 | GA-9680 | GA-9680B | |
| Penampilan | kulawu | Hideung | ||||||
| William plasticity | 160 | 180 | 200 | 220 | 240 | 270 | 270 | |
| Teu karasa (ShoreA) | 30 | 40 | 50 | 60 | 70 | 76 | 79 | |
| Kapadetan (g/cm3) | 2.1 | 2.13 | 2.15 | 2.2 | 2.25 | 2.04 | 2.35 | |
| Kakuatan tegangan (MPa) | 1 | 1.5 | 2 | 2 | 2.5 | 4.5 | 4.7 | |
| Elongation(%) | 800 | 750 | 700 | 600 | 500 | 80 | 130 | |
| Kakuatan cimata (kN/m) | 6 | 6 | 6 | 10 | 10 | 8 | 11.3 | |
| Koéfisién konduktivitas termal (W/MK) | 0.8 | 0.8 | 0.8 | 0.9 | 0.9 | 0.8 | 0.9 | |