Rabara ya fluorosilicone FV9500

sehlahiswa sena se loketse bakeng sa tlhahiso ya koloi turbocharger hose kapa tse ling tse motsoako hose le dihlahiswa tse ling.
Tiragatšo ye botse kudu ya go dira almanaka, tshepedišo ya go tlama yeo e fodišitšwego mmogo ka rabara ya silicone
Kganetšo ya oli ye botse kudu, go ganetša solvent.
  • FV9500 ya go swana le yona

  • Herchy ya go swana le

Go hwetšagala:
Palo: .

Ditšhupetšo tša setegeniki

Diaetheme

Ditšhupetšo

Kereiti

FV9540 ya go swana le

FV9550 ya go swana le

FV9560 ya go swana le

FV9561

Ponagalo

Mekgwa ya Teko

e serolane

Kgogedi ye e Itšego/ g/cm3

ASTM D792 ya go swana le yona

1.40

1.41

1.42

1.44

Go thatafala/lebopoA

ASTM D2240 ya go swana le yona

41

50

60

61

Matla a go goga/MPa

ASTM D412 ya go swana le yona

9.5

9.8

10.2

9.8

Elongation Ka Kgaotšo /% .

ASTM D412 ya go swana le yona

370

282

263

310

Matla a go gagoga/KN/m

ASTM D624-B ya go swana le yona

17

17

18

17

* Kganetšo ya Mocheso
225 ° C × 72h

Phetogo ya go thatafala /lebopong A

+4

+2

+2

+2

Phetogo ya maatla a go goga, % .

-24

-25

-23

-26

Elongation ka phetogo ya go kgaotša, % .

-19

-10

-14

-12

Mafura a C

Phetogo ya Bophagamo/% .

23 ° C / 72 h e

ASTM D471

+23

+23

+21

+21

Matla a Peel / N / mm, ka rabara ya silicone ya Methyl vinyl

2.0

2.0

2.2

2.0

Boemo bja go Fodiša

Oketša dikarolo tše 0.8 tša bis-di-quaternary, vulcanisation ya kgato e tee 120°C × 15min, vulcanisation ya kgato ye mebedi: 200°C × 4h


  • Kganetšo ya godimo go Ditikologo tše thata : Rabara ya fluorosilicone ya FV9500 e phala ditikologong tšeo di nago le dithemperetšha tše di feteletšego le go pepentšhwa dikhemikhale tše bogale. E nea go ganetša mo gobotse kudu go dibešwa, oli le dikhemikhale tše dintši, e lego seo se dirago gore e be e botse bakeng sa dikgopelo tše di nyakago tša intaseteri.

  • Wide Temperature Range : Thepa ena e fana ka e sephara tshebetso thempereichara fapaneng, ho tloha e tlase e le -60 ° C ho e phahameng e le 200 ° C. Se se dira gore e swanelege kudu bakeng sa dikgopelo diintasetering tša dikoloi, tša sefofane le tša tšweletšo, moo go feto-fetoga ga themperetšha go tlwaelegilego.

  • Excellent Compression Set Resistance : FV9500 bontša hlahelletseng ho hanyetsa ho compression sete, netefatsa nako e telele tshebetso le tiiso atleha tlas'a khatello e tšoarellang, esita le maemong a phahameng-khatello.

  • Enhanced Durability : Sebopego sa fluorosilicone se godiša go swarelela kgahlanong le botšofadi, ozone, le go pepentšhwa ga UV, go kgonthišetša go botega le go šoma ga nako ye telele, gaešita le ka fase ga maemo a tikologo a thata.

  • Superior Electrical Insulation : E fana ka thepa babatsehang motlakase kwahelang, ho etsa hore e loketseng bakeng sa ho sebelisoa ka dikarolo elektronike le tiiso dikopo moo ho hanyetsa motlakase ke bohlokoa.

  • Versatility ka Kopo : The thepa ka sebediswa ho pholletsa le liindasteri tse sa tšoaneng, ho akarelletsa le likoloi, sefofane, oli le khase, le elektronike, ka lebaka la motswako lona oa matla a mochine le ho hanyetsa lik'hemik'hale.

  • Go fetofetoga mo go botse le go ganetša go gagoga : Rabara ya fluorosilicone FV9500 e fana ka go fetofetoga le maemo le ge e le ka dithemperetšheng tša fase, go kopantšwe le go ganetša go gagoga le go gohla mo go botse kudu, go netefatša tshepedišo ye e ka botwago maemong a go fetoga le a godimo a go apara.

  • Dikgetho tša Mophato wa Dijo tše di lego gona : Go ya ka dinyakwa tša gago, mehuta ya raba ya fluorosilicone e ka hlangwa go fihlelela maemo a maemo a dijo, go fa tharollo ye e bolokegilego ya dikgopelo ka diintastering tša tshepedišo ya dijo le tša dihlare.


Peleng: 
Latelago: 

DIKGOKAGANO TŠA KA PELE

DIHLAHISWA TSA RONA

TSHEDIMOŠO YA KGOKAGANO

Add: No.33, Lane 159, Tsela ya Taiye, Setereke sa Fengxian, Shanghai
Mogala / WhatsApp / Skype: +86 15221953351 Mogala wa go swana le wa rena
Tokelo ya ngwalollo e ileditšwe     2023 Shanghai Herchy Rabara Co., Ltd. Mmapa wa Sebaka |   Pholisi ya Sephiri | Thekgo Ka Leadong ya go iša.