Rubber Fluorosilicone FV9500

He pai tenei hua mo te hanga o te ngongo turbocharger motuka, etahi atu ngongo hiato me etahi atu hua.
He pai te mahi whakamaarama, te mahi honohono tahi me te rapa silicone
He pai te atete hinu, te aukati whakarewa.
  • FV9500

  • Herchy

Wātea:
Rahi:

Tohu Hangarau

Nga taonga

Tohutohu

Kōeke

FV9540

FV9550

FV9560

FV9561

Te ahua

Nga Tikanga Whakamatau

kowhai

Te Kaha Tauwhāiti/ g/cm3

ASTM D792

1.40

1.41

1.42

1.44

Te pakeke/tatahiA

ASTM D2240

41

50

60

61

Te Kaha Toka/MPa

ASTM D412

9.5

9.8

10.2

9.8

Whakaroa I te Whati /%

ASTM D412

370

282

263

310

Te Kaha Roimata/KN/m

ASTM D624-B

17

17

18

17

*Atete Wea
225℃×72h

Huri pakeke / takutai A

+4

+2

+2

+2

Hurihia te kaha kaha, %

-24

-25

-23

-26

Te whakaroa i te huringa wehenga, %

-19

-10

-14

-12

Te hinu C

Huringa Rōrahi/%

23℃/72h

ASTM D471

+23

+23

+21

+21

Peel Strength/N/mm, with Methyl vinyl silicone rapa

2.0

2.0

2.2

2.0

Tikanga Whakaora

Tāpirihia kia 0.8 nga wahanga o te bis-di-quaternary, kotahi-waahanga whakangao 120℃×15min, rua-waahanga whakangao: 200℃×4h


  • Te Atete Nui ki nga Taiao Kino : FV9500 fluorosilicone rapa he pai ake i roto i nga taiao me te wera nui me te rongo ki nga matū kaha. He tino pai te aukati ki nga kora, nga hinu, me te tini o nga matū, e pai ana mo te tono tono ahumahi.

  • Awhe Paemahana Whanui : Ko tenei rauemi e tuku ana i te whānuitanga o te pāmahana whakahaere, mai i te iti -60°C ki te teitei ki te 200°C. Ma tenei ka tino pai mo nga tono i roto i nga miihini, aerospace, me nga umanga whakangao, kei reira nga rereketanga o te pāmahana.

  • Tino Pai te Whakataunga Whakataunga Whakapaipai : Ko te FV9500 e whakaatu ana i te tino atete ki te huinga huinga, e whakarite ana i te roa o te mahi me te pai o te hiri i raro i te pehanga pumau, ahakoa i roto i nga ahuatanga tino taumaha.

  • Whakanuia te Maamaa : Ko te hanganga fluorosilicone te whakanui ake i te kaha ki te koroheketanga, te ozone, me te whakaaturanga UV, me te whakarite i te pono mo te wa roa me te mahi, ahakoa i raro i nga tikanga taiao kino.

  • Te Hiko Hiko Nui : Ka whakaratohia e ia nga waahanga hiko hiko, he pai mo te whakamahi i nga waahanga hiko me nga tono hiri he mea nui te aukati hiko.

  • Te Whakamahinga i roto i te Whakamahinga : Ka taea te whakamahi i nga rauemi puta noa i nga momo ahumahi, tae atu ki te miihini, te aerospace, te hinu me te hau, me te hikohiko, na te whakakotahitanga o te kaha miihini me te aukati matū.

  • He pai te ngawari me te parenga roimata : Ko te rapa Fluorosilicone FV9500 e tuku ana i te ngawari ahakoa te iti o te mahana, me te pai o te roimata me te aukati abrasion, me te whakarite i te mahi pono i roto i nga ahuatanga hihiri me te kakahu teitei.

  • Nga Kōwhiringa Kai-Kai E waatea ana : I runga i o hiahia, ka taea te hanga i nga momo rapa fluorosilicone ki te whakatutuki i nga paerewa kai-kai, e whakarato ana i te otinga haumaru mo nga tono i roto i te tukatuka kai me nga ahumahi rongoa.


Tōmua: 
Panuku: 

NGA LINKO Tere

O TATOU HUA

HE KORERO WHAKAPAKI

Tāpirihia: No.33, Lane 159, Taiye Road, Takiwa Fengxian, Shanghai
Waea / WhatsApp / Skype: +86 15221953351
Ī-mēra:  info@herchyrubber.com
Mana pupuri     2023 Shanghai Herchy Rubber Co., Ltd. Mahere pae |   Kaupapahere Tūmataiti | Tautoko Na Leadong.