Tel: +8615221953351   E-mail: info@herchyrubber.com
PRODUCTS
You are here: Home » Products » Synthesis Rubber » FVMQ Fluorosilicone » Fluorosilicone Rubber FV9500

loading

Share to:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
sharethis sharing button

Fluorosilicone Rubber FV9500

This product is suitable for the production of automotive turbocharger hose or other composite hose and other products.
Excellent calendering performance, co-cured bonding performance with silicone rubber
Excellent oil resistance, solvent resistance.
  • FV9500

  • Herchy

Availability:
Quantity:

Technical indicators

Items

Indicators

Grade

FV9540

FV9550

FV9560

FV9561

Appearance

Test Methods

yellowish

Specific Gravity/ g/cm3

ASTM D792

1.40

1.41

1.42

1.44

Hardness/shoreA

ASTM D2240

41

50

60

61

Tensile Strength/MPa

ASTM D412

9.5

9.8

10.2

9.8

Elongation At Break /%

ASTM D412

370

282

263

310

Tear Strength/KN/m

ASTM D624-B

17

17

18

17

*Heat Resistance
225℃×72h

Hardness change /shore A

+4

+2

+2

+2

Tensile strength change, %

-24

-25

-23

-26

Elongation at break change, %

-19

-10

-14

-12

Fuel C

Volume Change/%

23℃/72h

ASTM D471

+23

+23

+21

+21

Peel Strength/N/mm, with Methyl vinyl silicone rubber

2.0

2.0

2.2

2.0

Curing Condition

Add 0.8 parts of bis-di-quaternary, one-stage vulcanisation 120℃×15min, two-stage vulcanisation: 200℃×4h


  • Superior Resistance to Harsh Environments: FV9500 fluorosilicone rubber excels in environments with extreme temperatures and exposure to aggressive chemicals. It provides excellent resistance to fuels, oils, and a wide range of chemicals, making it ideal for demanding industrial applications.

  • Wide Temperature Range: This material offers a broad operating temperature range, from as low as -60°C to as high as 200°C. This makes it highly suitable for applications in automotive, aerospace, and manufacturing industries, where temperature fluctuations are common.

  • Excellent Compression Set Resistance: FV9500 demonstrates outstanding resistance to compression set, ensuring prolonged performance and sealing effectiveness under sustained pressure, even in high-stress conditions.

  • Enhanced Durability: The fluorosilicone composition enhances durability against aging, ozone, and UV exposure, ensuring long-term reliability and performance, even under harsh environmental conditions.

  • Superior Electrical Insulation: It provides excellent electrical insulation properties, making it ideal for use in electronic components and sealing applications where electrical resistance is crucial.

  • Versatility in Application: The material can be used across various industries, including automotive, aerospace, oil and gas, and electronics, due to its combination of mechanical strength and chemical resistance.

  • Good Flexibility and Tear Resistance: Fluorosilicone rubber FV9500 offers flexibility even at low temperatures, combined with excellent tear and abrasion resistance, ensuring reliable performance in dynamic and high-wear conditions.

  • Food-Grade Options Available: Depending on your requirements, fluorosilicone rubber variants can be formulated to meet food-grade standards, providing a safe solution for applications in food processing and pharmaceutical industries.


Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.