FV9700
Hercsekele
| Boteng: | |
|---|---|
| Bongata: | |
Ntho |
Lipontšo |
||
Nomoro ea letoto |
NFS9760 |
NFS9770 |
|
Ponahalo Mekhoa ea Tlhahlobo |
Sebaka se phatsimang, se boreleli, Ha ho litšila |
||
Matla a khoheli a khethehileng/ g/cm3 |
ASTM D792 |
1.44 |
1.48 |
Ho thatafala/lebopoA |
ASTM D2240 |
60 |
70 |
Tensile Strength/MPa |
ASTM D412 |
10.5 |
10.1 |
Elongation At Break /% |
ASTM D412 |
207 |
201 |
Matla a ho lla/KN/m |
ASTM D624-B |
18 |
17 |
Compress Set(177℃*22h) |
Hardness variation/A |
+4 |
+5 |
Sekhahla sa phetoho ea matla a tensile/% |
-27 |
-24 |
|
Sekhahla sa phetoho ea bolelele/% |
-26 |
-23 |
|
Mafura C Phetoho ea Bolumo/% 23℃/72h |
ASTM D471 |
21 |
20 |
IRM903 |
ASTM D471 |
4.5 |
4 |
Asiti ea nitric/sulfuric acid/hydrochloric acid e tsoakiloeng PH<1 100℃×120h |
|||
Acid resistance |
ASTM D471 |
0.3 |
0.3 |
3% tharollo ea sodium hydroxide 60 ℃×72h |
|||
Alkali resistance |
ASTM D471 |
0.4 |
0.3 |
Phekolo Boemo |
0.8 likarolo tsa bisditetra, vulcanisation ea mohato o le mong 120 ℃×15min, vulcanisation ea mekhahlelo e 'meli: 200 ℃×4h |
||
Ketso tse khothalelitsoeng:
Ho khothaletsoa ho sebelisa likarolo tse 0.4-0.7 tsa bisdisulfide (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).
Bareki ba lokela ho khetha mocheso o nepahetseng ka ho fetisisa le nako ea ho phekola ho latela boholo ba sehlahisoa le mokhoa oa ho phekola.
Sephutheloana sa sehlahisoa:
Sehlahisoa sena ha se kotsi, ho e-na le hoo se entsoe ka cardstock, polasetiki, le lik'hilograma tse 10 ka mokotla, mekotla e 2 ka lebokose.
Lilemo tsa polokelo:
Sehlahisoa sena se na le matla a ho phalla a batang, mokotla o lokela ho qojoa e le hore o se ke oa senyeha nakong ea lipalangoang kapa ho sebelisoa.
Boloka sebakeng se pholileng, se omeletseng se nang le sethala sa bophelo ba likhoeli tse 12.