FV9700 Fluorosilicone hmanga siam a ni

He product hi bis-disulfide extrusion molding atan a tha hle. Oil resistance tha tak a nei a, solvent resistance tha tak a nei a, acid leh alkali resistance tha tak a nei bawk.
  • FV9700 a ni

  • Herchy a ni

A awm theihna:
A zat:

Technical lam hawi thilte



Thil

Indicators te pawh a awm

Serial number a ni

NFS9760 a ni

NFS9770 a ni

Landan

Test dan tur

Translucent, a chung lam hrual, .

Thil bawlhhlawh a awm lo

Gravity bik/ g/cm a ni3

ASTM D792 a ni

1.44

1.48

Hardness/shoreA tih a ni

ASTM D2240 a ni

60

70

Tensile chakna/MPa

ASTM D412 a ni

10.5

10.1

Elongation At Break /% a ni.

ASTM D412 a ni

207

201

Mittui chakna/KN/m

ASTM D624-B a ni

18

17

A rilru a buai em em a, a rilru a hah em em bawk a. 177°C*22h)

Hardness danglamna/A

+4

+5

Tensile strength inthlak danglamna rate/% 1.1.

-27

-24

Elongation inthlak danglamna rate/% .

-26

-23

Fuel C. a ni

Volume inthlak danglamna/%

23°C/72h a ni

ASTM D471 a ni

21

20

IRM903
Volumetric rate inthlak danglamna/%
150°C×72h

ASTM D471 a ni

4.5

4

Nitric acid/sulfuric acid/hydrochloric acid inzawmkhawm PH2 100°C×120h

Acid laka invenna
Volume inthlak danglamna rate/% .

ASTM D471 a ni

0.3

0.3

3% sodium hydroxide solution 60°C×72h a awm tur a ni

Alkali laka invenna
Volume inthlak danglamna rate/% .

ASTM D471 a ni

0.4

0.3

Curing Condition a ni

Bisditetra hmun 0.8, vulcanisation stage khata 120°C×15min, vulcanisation stage hnih: 200°C×4h

Thil tih tur rawtna: 1.1.


Bisdisulfide (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane) 0.4-0.7 vel hman a rawt a ni.


Customer te chuan an thil siam lian leh te, an tihdam dan a zirin temperature leh hun remchang ber an thlang tur a ni.


Product packaging hrang hrang: 1.1.


He thil hi a hlauhawm lo a, chu ai chuan cardstock, plastic, leh bag khatah kilogram 10, box khatah bag 2 atanga siam a ni.


A dahna kum: 1.1.


He product hian cold flow capacity a nei a, bag hi a phurh chhuah emaw hman lai emaw a chhiat loh nan pumpelh tur a ni.


Thla 12 chhung a awm theihna tur hmun lum leh vawt takah dah tur a ni.


Hma chiah: 
Dawtchiah: 

QUICK LINKS A AWM VE ANG

CONTACT THIL AWM DAN

Add: No.33, Lane 159, Taiye kawngpui, Fengxian District, Shanghai-a awm a ni
Tel / WhatsApp / Skype: +86 15221953351 ah zawhfiah theih a ni
E-mail hmangin:  info@herchyrubber.com
A rilru a hah   lutuk chuan a rilru   2023 a buai em em a. Shanghai Herchy Rubber Co., Ltd. Sitemap a ni |   Thuruk humhalh dan tur | Support By Leadong a ni.