FV9700 Fluorosilicone

Alaabtani waxay ku habboon tahay naqshadaynta extrusion ee bis-disulfide. Waxay leedahay iska caabin saliid heer sare ah, caabbinta dareeraha, caabbinta acid iyo alkali.
  • FV9700

  • Herchy

Helitaanka:
Tirada:

Tilmaamayaasha farsamada



Shayga

Tilmaamayaal

Nambarka taxanaha ah

NFS9760

NFS9770

Muuqashada

Hababka Imtixaanka

Oogada dhalaalaysa, siman,

Wax wasakh ah ma leh

Cufis-jiidad gaar ah/g/cm3

ASTM D792

1.44

1.48

Adag/xerigaA

ASTM D2240

60

70

Xoojinta Xoojinta/MPa

ASTM D412

10.5

10.1

Kordhinta Waqtiga Nasashada /%

ASTM D412

207

201

Xoog jeexjeexa/KN/m

ASTM D624-B

18

17

Qaabka cadaadiska (177℃*22h)

Kala duwanaanta adagaanta/A

+4

+5

Heerka isbeddelka xoogga xajinta/%

-27

-24

Heerka isbeddelka dhererka/%

-26

-23

Shidaalka C

Bedelka codka /%

23 ℃/72saac

ASTM D471

21

20

IRM903
Heerka cabbirka isbeddelka/%
150 ℃×72h

ASTM D471

4.5

4

Nitric acid/sulfuric acid/hydrochloric acid xal isku dhafan PH<1 100℃×120h

Iska caabbinta aysiidhka Heerka
isbeddelka mugga/%

ASTM D471

0.3

0.3

3% sodium hydroxide xal 60 ℃ × 72h

Iska caabbinta Alkali Heerka
isbeddelka mugga/%

ASTM D471

0.4

0.3

Xaalada Caafimaad

0.8 qaybood oo bisditetra ah, vulcanisation hal-heer ah 120 ℃ × 15min, laba marxaladood vulcanisation: 200 ℃ × 4h

Ficilada lagu taliyay:


Waxaa la soo jeediyay in la isticmaalo 0.4-0.7 qaybaha bisdisulfide (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).


Macaamiishu waa inay doortaan heerkulka ugu habboon iyo wakhtiga daawaynta iyadoo lagu salaynayo cabbirka badeecada iyo habka daawaynta.


Baakadaha alaabta:


Alaabtani maaha mid khatar ah, waxay ka kooban tahay kartoon, balaastiig, iyo 10 kiilogaram halkii bac, 2 bacdiiba sanduuqii.


Da'da kaydinta:


Alaabtani waxay leedahay awood socodka qabow, bacda waa in laga fogaadaa si aysan u dhaawacmin inta lagu jiro gaadiidka ama isticmaalka.


Ku hay meel qabow oo qalalan oo cimrigeedu shelf yahay 12 bilood.


Kii hore: 
Xiga: 

XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.