Sɔhwɛ: A/B nsusuwii a ɛyɛ 1 :1, 130 ° C x 5min x 15MPa
| Nneɛma a wɔyɛ no parameters | |||||||
| Adwadeɛ | GA-2720 na ɛwɔ hɔ | GA-2730 na ɛwɔ hɔ | GA-2740 na ɛwɔ hɔ | GA-2750 na ɛwɔ hɔ | GA-2760 na ɛwɔ hɔ | GA-2770 na ɛwɔ hɔ | |
| Mmaeɛ | Fann | ||||||
| Nsuo a ɛyɛ den(Pa.s) . |
2000 | 3000 | 3000 | 3500 |
4000 | 5000 |
|
| Nneɛma a ɛyɛ den (ShoreA) . | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Nsuo a ɛyɛ den(g/cm3) . | 1.10 | 1.10 | 1.11 | 1.12 | 1.1.3 |
1.14 |
|
| Ahoɔden a wɔde twe ade (MPa) . | 7.0 |
8.0 |
9.5 |
10.0 |
10.0 |
9.5 |
|
| Ntrɛwmu(%) . | 880 | 800 | 700 | 550 | 500 |
350 |
|
| Ahoɔden a ɛtetew mu (kN/m) . | 16 | 30 | 35 |
40 | 35 |
30 |
|
| Ntrɛwmu a ɛkɔ soro(%) . | 2.1 | 2.1 | 2.1 | 2.0 | 2.0 |
2.0 |
|