GA-2033 Rabara ea Silicone e itšebetsang (LSR)

Kopo: e loketse ho hlahisa likarolo tsa likoloi, plug, joalo-joalo.
Likarolo tsa bohlokoa: matla a phahameng, thepa e ntle ea ho tsoa mali a oli.
  • GA-2033

  • Herchy

Boteng:
Bongata:

Teko: A/B karo-karolelano ea 1 :1, 130°C x 5min x 15MPa

Lihlahisoa tsa lihlahisoa
Sehlahisoa GA-2033
GA-2043 GA-2053 GA-2045
Ponahalo Translucent
Viscosity(Pa.s)
2000 3000 4000 3500
Ho thatafala (LebopoA) 30 40 50
40
Boima ba 'mele(g/cm3) 1.10 1.12 1.14 1.13
Tensile Matla (MPa) 6.5
8.0
9.5
7.5
Elongation(%) 650 550 500 550
Matla a ho lla (kN/m) 13 20 27
21
Linearshrinkage(%) 1.8 1.8 1.8 1.8
Compressionset 175 x 22H (%) -
-
-
20










E fetileng: 
E 'ngoe: 

LIEKETSENG POTLAKO

LIHLAHISO TSA RONA

MOKHOA OA PUISANO

Eketsa: No.33, Lane 159, Taiye Road, Setereke sa Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sebaka sa marang-rang |   Leano la Lekunutu | Tšehetso Ka Leadong.