GA-200X None Post-curing Liquid Silicone Rubber (LSR)

Kopo: e loketse ho hlahisa sehlahisoa sa masea, joalo ka, nipple ea lesea, botlolo ea lesea, joalo-joalo.
Likarolo tsa bohlokoa: taba e sa fetoheng, pepeneneng e phahameng, thepa e ntle ea mochini, fetisa netefatso ea RoHS, REACH, FDA, le LFGB
  • GA-2002

  • Herchy

Ho fumaneha:
Bongata:

Teko: A/B karo-karolelano ea 1 :1, 130°C x 5min x 15MPa


Lihlahisoa tsa lihlahisoa
Sehlahisoa GA-2002 GA-2003 GA-2004 GA-2005 GA-2006 GA-2007
Ponahalo Tse pepeneneng

Ho thatafala (LebopoA) 23 30 40 50
62
68
Boima ba 'mele(g/cm3) 1.10 1.12 1.12 1.13 1.14
1.14
Tensile Matla (MPa) 6.0
8.0
9.0
9.0
10.0
9.5
Elongation(%) 750 650 600 500 450
400
Matla a ho lla (kN/m) 10 15 20
25 30
35
Litaba tsa VOC(%) 0.35 0.35 0.3 0.3 0.3 0.3







E fetileng: 
E 'ngoe: 

LIEKETSENG POTLAKO

LIHLAHISO TSA RONA

MOKHOA OA PUISANO

Eketsa: No.33, Lane 159, Taiye Road, Setereke sa Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sebaka sa marang-rang |   Leano la Lekunutu | Tšehetso Ka Leadong.