Motsoako oa rabara oa EPDM/EPM kapa precompound-EPDM/EPM
Ethylene propylene rubber is a synthetic rubber with ethylene and propylene as the main monomer, according to the different composition of the monomer in the molecular chain, there are binary ethylene propylene rubber and tertiary ethylene propylene rubber, the former is a copolymer of ethylene and propylene, to EPM, the latter is a copolymer of ethylene, propylene le palo e nyane ea non-conjugated diolefin monomer ea boraro, ho EPM. Ka bobeli li tsejoa ka kakaretso e le rabara ea ethylene propylene, kapa rabara ea ethylene propylene (EPR). E sebelisoa haholo likarolong tsa likoloi, lisebelisoa tse sa keneleng metsi bakeng sa kaho, terata le ho roala ka mohala, li-hoses tse sa keneleng mocheso, litheipi, litiiso tsa likoloi, lisebelisoa tsa lubricant le lihlahisoa tse ling.
Tshebetso:
1, Boima bo tlaase le ho tlatsa holimo
2, Ho hanyetsa botsofali bo botle
3. Corrosion resistance
4. Ho hanyetsa mouoane oa metsi
5, ho hanyetsa metsi a chesang haholo
6, Ts'ebetso e ntle ea motlakase
7, Elasticity e Ntle
Herchy Rubber e na le sehlopha sa R&D se nang le boiphihlelo ba lilemo tse fetang 10 ho kopantseng EPDM.
Motsoako oa EPDM oa Herchy Rubber o sebelisoa haholo indastering ea likoloi, ho tiisa kaho, lisebelisoa tsa ntlo, terata le thapo, lirolara tsa rabara, lithaere le liindasteri tse ling.
| Herchy | Mofuta oa vulcanization | Mooney viscosity | Ho thatafala | Matla a tšepe | Elongation nakong ya khefu | 125 ℃ * 72h Botsofali bo futhumetseng | Compress set | Kopo | Sebopeho | ||
| Phetoho ea boima | Phetoho ea matla | Phetoho ea bolelele | 125℃*72h ASTM D395 Mofuta oa B | ||||||||
| Kereiti | ML(1+4)100℃ | Shore A | Mpa | % | Shore A | % | % | % | |||
| EPDM-S5060 | Sebabole | 50 | 60 | mets.10 | mets.300 | boholo.+10 | boholo.-25 | boholo.-25 | boholo.50 | Lihlahisoa tse fetisitsoeng, lihlahisoa tse kentsoeng, lihlahisoa tse bōpiloeng | Boleng bo botle; |
| EPDM-S6060 | Sebabole | 60 | 60 | mets.10 | mets.300 | boholo.+10 | boholo.-25 | boholo.-25 | boholo.50 | Lihlahisoa tse fetisitsoeng, lihlahisoa tse kentsoeng, lihlahisoa tse bōpiloeng | Boleng bo botle; |
| EPDM-S7060 | Sebabole | 70 | 60 | mets.10 | mets.300 | boholo.+10 | boholo.-25 | boholo.-25 | boholo.50 | Lihlahisoa tse fetisitsoeng, lihlahisoa tse bōpiloeng | Matla a phahameng a mochini; |
| EPDM-S8060 | Sebabole | 80 | 60 | mets.10 | mets.300 | boholo.+10 | boholo.-25 | boholo.-25 | boholo.50 | Lihlahisoa tse fetisitsoeng, lihlahisoa tse bōpiloeng | Matla a phahameng a mochini; |
| EPDM-P5060 | Peroxide | 50 | 60 | mets.10 | mets.200 | boholo.+5 | boholo.-20 | boholo.-20 | boholo.30 | Lihlahisoa tse fetisitsoeng, lihlahisoa tse kentsoeng, lihlahisoa tse bōpiloeng | Boleng bo botle; Ho hanyetsa mocheso o phahameng; Tlaase Compression set |
| EPDM-P6060 | Peroxide | 60 | 60 | mets.10 | mets.200 | boholo.+5 | boholo.-20 | boholo.-20 | boholo.30 | Lihlahisoa tse fetisitsoeng, lihlahisoa tse kentsoeng, lihlahisoa tse bōpiloeng | Ho hanyetsa mocheso o phahameng; Boleng bo botle; Tlas'a Compression set; |
| EPDM-P7060 | Peroxide | 70 | 60 | mets.10 | mets.200 | boholo.+5 | boholo.-20 | boholo.-20 | boholo.30 | Lihlahisoa tse fetisitsoeng, lihlahisoa tse bōpiloeng | Ho hanyetsa mocheso o phahameng; Matla a phahameng a mochine; Low Compression set; |
| EPDM-P8060 | Peroxide | 80 | 60 | mets.10 | mets.200 | boholo.+5 | boholo.-20 | boholo.-20 | boholo.30 | Lihlahisoa tse fetisitsoeng, lihlahisoa tse bōpiloeng | Ho hanyetsa mocheso o phahameng; Matla a phahameng a mochine; Low Compression set; |
1, Lesela la tiiso ea rabara ea koloi
Ho hanyetsa boemo ba leholimo bo botle, ho hanyetsa ozone, ho hanyetsa mocheso, ho hanyetsa acid le alkali, ho hanyetsa mouoane oa metsi, botsitso ba mebala, thepa ea motlakase, ho tlala oli le mocheso oa kamore.
Khothalletsa: EPDM:S512F;S5890F;S552;S552-1;S553;S5206F;S5527F;S6090WF;S 600WF;S7486F;S6075WF;3062E;J-3060P;J-3080;J-3080P;J-3092E;J-4090;TER 4033;TER 4038EP;TER 4039;TER 4044;TER 4049;TER 4334;TER 6148;TER 6235;TER 6537;TER 9046;TER 8148;TER 7040;TER 4049;TER 5029;
2, Hose
Ho hanyetsa hantle lik'hemik'hale tse fapaneng tsa polar tse kang joala, li-acids, alkalis, oxidizers, lihatsetsi, li-detergents, oli ea liphoofolo le ea meroho, ketone le mafura.
Khothalletsa: EPDM:S512F;S5890F;S552;S552-1;S6090WF;J-3060P;J-3080;J-3080P;J-3092E;TER 4038EP;TER 4039;TER 4049;TER 4047;
3, thapo ea mohala
Ho hanyetsa boemo ba leholimo bo botle, ho hanyetsa ozone, ho hanyetsa mocheso.Ethylene propylene rabara e na le thepa e babatsehang ea ho kenya motlakase le ho hanyetsa corona, thepa ea motlakase e molemo ho feta kapa e haufi le rabara ea styrene butadiene, chlorosulfonated polyethylene, polyethylene le polyethylene e amanang le sefapano.
Khothalletsa: EPDM:S505A;S512F;3062E;J-3060P;TER 4033;TER 4044
4, O-rings
Ka lebaka la khaello ea polarity le tlase unsaturation ea ethylene propylene rabara, e na le ho hanyetsa e ntle ho lik'hemik'hale tse sa tšoaneng polar tse kang joala, acid, alkalis, oxidizers, refrigerants, detergents, liphoofolo le oli ea meroho, ketone le mafura.
Khothalletsa:EPDM:S552;S552-1;S512F;TER 4049;TER 4047;TER 4039;TER 4038EP;J-3092E;J-3080;J-3080P
5. Lera le sa keneleng metsi
Ho hanyetsa boemo ba leholimo bo botle, ho hanyetsa ozone, ho hanyetsa mocheso, ho hanyetsa acid le alkali, ho hanyetsa mouoane oa metsi, botsitso ba mebala, thepa ea motlakase, ho tlala oli le mocheso oa kamore.
Khothalletsa:TER 4334;CO 054;3062E;S537-2;S501A;S537-3;S5890F;
6. Rolara ea rabara
Ka lebaka la khaello ea polarity le tlase unsaturation ea ethylene propylene rabara, e na le ho hanyetsa e ntle ho lik'hemik'hale tse sa tšoaneng polar tse kang joala, acid, alkalis, oxidizers, refrigerants, detergents, liphoofolo le oli ea meroho, ketone le mafura.
Khothalletsa:EPDM:S501A;S505A;3062E;J-2080;TER 4047;TER 4334;TER 4039;
7 Tyre
Ho hanyetsa boemo ba leholimo bo botle, ho hanyetsa ozone, ho hanyetsa mocheso, ho hanyetsa acid le alkali, ho hanyetsa mouoane oa metsi, botsitso ba mebala, thepa ea motlakase, ho tlala oli le mocheso oa kamore.
Khothalletsa: EPDM:S537-3;S537-2;S505A;J-2080;J-2070;TER 4047;
8, Lithako tsa Rubber tsa Shoe
Ho hanyetsa boemo ba leholimo bo botle, ho hanyetsa ozone, ho hanyetsa mocheso, ho hanyetsa acid le alkali, ho hanyetsa mouoane oa metsi, botsitso ba mebala, thepa ea motlakase, ho tlatsoa ka oli le mocheso oa kamore. Kaha ha ho na sebaka sa polar mohahong oa limolek'hule oa rabara ea ethylene propylene, matla a ho kopana ha limolek'hule a tlaase, 'me ketane ea molek'hule e ka boloka ho fetoha ha maemo ho ea ka mefuta e mengata ea rabara, ea bobeli e ka boloka rabara e le tlase, ea bobeli e ka boloka rabara e le tlase. mocheso.
Khothalletsa:
EPDM:S537-3;S537-2;J-2070;J-2080;TER 6235;TER 4548;