Kopo: e loketse ho hlahisa libethe tsa setempe tse chesang, poleiti e chesang ea setempe, rolara ea ho fetisa e chesang, copier roller, joalo-joalo.
Likarolo tsa bohlokoa: khanyetso e ntle ho mocheso o phahameng le o tlase (60 'C -350 'C), ho tiea ho hoholo le ho hanyetsa ho hoholo ho hoholo, sete e tlase ea deformation, ho thata ho holofala le ho robeha, bophelo bo bolelele ba ts'ebeletso.
Teko: 1% ea moemeli oa ho folisa (50% peista ea DBPMH ka har'a chese ea silicone), 175'C x 5min x 15MPa.
| Lihlahisoa tsa lihlahisoa | ||||||
| Sehlahisoa | GA-5750 | GA-5770 | GA-5780 | GA-5741 | GA-5761 | |
| Ponahalo | Hoary | E mosehla | ||||
| Ho thatafala (LebopoA) | 55 | 70 | 80 | 43 | 60 | |
| Tensile Matla (MPa) | 5.5 | 6 | 7 | 6 | 8 | |
| Elongation(%) | 230 | 150 | 100 | 400 | 350 | |
| Matla a ho lla (kN/m) | 10 | 9 | 9 | 15 | 25 | |
| 175'C x22h Compression(%) | 8 | 10 | 10 | 10 | 10 | |