GA-2618G Liquid Silicone Rubber yeBaby Nipple yeNew GB (LSR)

Application: mwana zamu.
Akakosha maficha: kujeka kwepamusoro, yakanakisa michina chivakwa, inoenderana neGB38995-2020 yemabhodhoro ekudyisa vacheche uye mateti, pfuura humbowo hweRo HS, 0 REACH, FDA, uye LFGB.
  • GA-2618G

  • Herchy

Kuwanikwa:
Huwandu:

Muedzo: A/B reshiyo ye1 :1, 130°C x 5min x 15MPa


Product parameters
Product GA-2618G GA-2620G GA-2625G
Chitarisiko Transparent
Kuoma (ShoreA) 18 22 25
Density(g/cm3) 1.10 1.10 1.10
Tensile simba (MPa) 6.5
7.5
7.5
Elongation(%) 900 850 800
Simba rekubvarura (kN/m) 20 22
22







Zvakapfuura: 
Zvinotevera: 

KUKURUMIDZA ZVINONYANYA

ZVINHU ZEDU

CONTACT INFORMATION

Wedzera: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.