GA-2618G kan jedhu
Herchy jedhamuun beekama
| Argamuu: | |
|---|---|
| Baay’ina: | |
Qormaata: Reeshiyoon A/B 1 :1, 130°C x 5min x 15MPa
| Parameetaroota oomishaa | ||||
| Oomisha | GA-2618G kan jedhu | GA-2620G jedhamuun beekama | GA-2625G irratti kan hundaa’e | |
| Mul'ina | Of keessa dabarsuu | |||
| Jabina (ShoreA) . | 18 | 22 | 25 |
|
| Dandeettii(g/cm3) . | 1.10 | 1.10 | 1.10 | |
| Jabina harkisaa (MPa) . | 6.5 |
7.5 |
7.5 |
|
| Dheersuu(%) . | 900 | 850 | 800 | |
| Jabina ciccituu (kN/m) . | 20 | 22 |
22 |
|