GA-2618G
Herchy
| Upatikanaji: | |
|---|---|
| Kiasi: | |
Jaribio: Uwiano wa A/B wa 1 :1, 130°C x 5min x 15MPa
| Vigezo vya bidhaa | ||||
| Bidhaa | GA-2618G | GA-2620G | GA-2625G | |
| Muonekano | Uwazi | |||
| Ugumu (ShoreA) | 18 | 22 | 25 |
|
| Msongamano(g/cm3) | 1.10 | 1.10 | 1.10 | |
| Nguvu ya mkazo (MPa) | 6.5 |
7.5 |
7.5 |
|
| Kurefusha(%) | 900 | 850 | 800 | |
| Nguvu ya machozi (kN/m) | 20 | 22 |
22 |
|