GA-2618G
Herchy
| Dobavljivost: | |
|---|---|
| Količina: | |
Test: razmerje A/B 1:1, 130 °C x 5 min x 15 MPa
| Parametri izdelka | ||||
| Izdelek | GA-2618G | GA-2620G | GA-2625G | |
| Videz | Transparentna | |||
| Trdota (ShoreA) | 18 | 22 | 25 |
|
| Gostota (g/cm3) | 1.10 | 1.10 | 1.10 | |
| Natezna trdnost (MPa) | 6.5 |
7.5 |
7.5 |
|
| Raztezek (%) | 900 | 850 | 800 | |
| Trdna trdnost (kN/m) | 20 | 22 |
22 |
|