GA-2618G Liquid Silicone Rubber maka Nwa ara ara nke GB ọhụrụ (LSR)

Ngwa: nwa ara.
Akụkụ ndị dị mkpa: nghọta dị elu, akụrụngwa akụrụngwa dị mma, kwekọrọ na GB38995-2020 maka karama na-enye nri nwa ọhụrụ, gafere nkwenye nke Ro HS,0 REACH, FDA, na LFGB.
  • GA-2618G

  • Herchy

Nnweta:
Ọnụọgụ:

Nnwale: Oke A/B nke 1:1, 130°C x 5min x 15MPa


Ngwa ngwaahịa
Ngwaahịa GA-2618G GA-2620G GA-2625G
Ọdịdị N'ụzọ doro anya
Isi ike (ShoreA) 18 22 25
Njupụta (g/cm3) 1.10 1.10 1.10
Ike tensile (MPa) 6.5
7.5
7.5
Mgbatị(%) 900 850 800
Ike akwa mmiri (kN/m) 20 22
22







Nke gara aga: 
Osote: 

Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nwebiisinka     2023 Shanghai Herchy Rubber Co., Ltd. map saịtị |   Amụma nzuzo | Nkwado Site Leadong.