Ujian: Nisbah A/B 1 :1, 130°C x 5min x 15MPa
| Parameter produk | ||||
| produk | GA-2618G | GA-2620G | GA-2625G | |
| Penampilan | Telus | |||
| Kekerasan (ShoreA) | 18 | 22 | 25 |
|
| Ketumpatan(g/cm3) | 1.10 | 1.10 | 1.10 | |
| Kekuatan tegangan (MPa) | 6.5 |
7.5 |
7.5 |
|
| Pemanjangan(%) | 900 | 850 | 800 | |
| Kekuatan koyakan (kN/m) | 20 | 22 |
22 |
|