GA-2340
Herchy
| Kuwanikwa: | |
|---|---|
| Huwandu: | |
Muedzo: AB reshiyo ye10:1 kana 1:1, 130'C x 5min x 15Mpa.
| Product parameters | |||
| Product | GA-2340 |
GA-2341 | |
| Chitarisiko | Translucent | ||
| A/Bratio | A:B=10:1 |
A:B=1:1 |
|
| Viscosity(Pa.s) |
50/1 | 75/75 | |
| Kuoma (ShoreA) | 38 | 38 | |
| Density(g/cm3) | 1.08 | 1.08 | |
| Tensile simba (MPa) | 6.5 |
6.5 |
|
| Elongation(%) | 400 | 400 | |
| Simba rekubvarura (kN/m) | 18 | 18 | |
| Linearshrinkage(%) | 2.0 |
2.0 | |