Ucingo: +86 15221953351 I-imeyili: info@herchyrubber.com
Please Choose Your Language
IMIKHIQIZO
Ulapha: Ikhaya » Imikhiqizo » Irabha Yokuhlanganisa » I-Silicone ye-VMQ GA -2618G Liquid Silicone Rubber for Baby Nipple of New GB (LSR)

iyalayisha

Yabelana ku-:
inkinobho yokwabelana ye-facebook
inkinobho yokwabelana ye-twitter
inkinobho yokwabelana ngomugqa
inkinobho yokwabelana ye-wechat
inkinobho yokwabelana ye-linkedin
inkinobho yokwabelana ye-pinterest
inkinobho yokwabelana ye-whatsapp
yabelana ngale nkinobho yokwabelana

I-GA-2618G Liquid Silicone Rubber ye-Baby Nipple of New GB (LSR)

Isicelo: ingono yengane.
Izici ezibalulekile: ukukhanya okuphezulu, indawo enhle kakhulu yomshini, ethobela i-GB38995-2020 yamabhodlela okuncelisa izinsana kanye nebele, kuphumelele ukuqinisekiswa kwe-Ro HS, 0 REACH, FDA, kanye ne-LFGB.
  • I-GA-2618G

  • I-Herchy

Ukutholakala:
Ubuningi:

Isivivinyo: A/B isilinganiso 1 :1, 130°C x 5min x 15MPa


Imingcele yomkhiqizo
Umkhiqizo I-GA-2618G I-GA-2620G I-GA-2625G
Ukubukeka Okusobala
Ukuqina (ShoreA) 18 22 25
Ukuminyana(g/cm3) 1.10 1.10 1.10
Amandla e-Tensile (MPa) 6.5
7.5
7.5
Ubude(%) 900 850 800
Amandla wezinyembezi (kN/m) 20 22
22







Okwedlule: 
Olandelayo: 

IZIXHUMANISI EZISHESHAYO

IMIKHIQIZO YETHU

ULWAZI LOKUXHUMANA

Engeza: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Ucingo / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Imephu yesayithi |   Inqubomgomo Yobumfihlo | Sekela Ngu I-Leadong.