Langi: Black
Obukaluba: 55-65 Shore A
Enkola ya Vulcanization: enkola ya sulfur
Raw rubber acrylonitrile content: 35±3%
Size: esobola okulongoosebwa (strip oba wide)
Embeera za Vulcanization: 170 ° C * 10min secondary vulcanization: 150 ° C * 4h (2mm standard test piece)