GA-2002
Herchy nga bwe kiri
| Okubeerawo: | |
|---|---|
| Omuwendo: | |
Okugezesa: Omugerageranyo gwa A/B gwa 1 :1, 130°C x 5min x 15MPa
| Ebipimo by’ebintu ebikolebwa | |||||||
| Ekyamaguzi | GA-2002 | GA-2003 | GA-2004 | GA-2005 | GA-2006 | GA-2007 | |
| Endabika | Okutangaala | ||||||
| Obukaluba (ShoreA) . | 23 | 30 | 40 | 50 |
62 |
68 |
|
| Obugumu(g/cm3) . | 1.10 | 1.12 | 1.12 | 1.13 | 1.14 |
1.14 |
|
| Amaanyi g’okusika (MPa) . | 6.0 |
8.0 |
9.0 |
9.0 |
10.0 |
9.5 |
|
| Okuwanvuwa(%) . | 750 | 650 | 600 | 500 | 450 |
400 |
|
| Amaanyi g’okukutuka (kN/m) . | 10 | 15 | 20 |
25 | 30 |
35 |
|
| Ebirimu VOC(%) . | 0.35 | 0.35 | 0.3 | 0.3 | 0.3 | 0.3 | |