Fluorosilicone Omupiira FV9200

Ekintu kino kitabuddwamu ekizigo ekikoleddwa mu fluorosilicone nga kirimu ebirungo eby’enjawulo ebigiyamba n’okujjuza.
Amaanyi g’okusika aga waggulu aga waggulu n’obulungi bw’amaziga obw’amaanyi.
Okugumira amafuta mu ngeri ey’ekitalo, okugumira ekisengejja n’okugumira ebbugumu erya waggulu n’erya wansi.
  • FV9200

  • Herchy .

Ebiriwo:
Omuwendo:




Ebintu


Ebiraga

Ebigezo

FV9240

FV9250

FV9260

Enkola z’okugezesa / Endabika

Enjeru ng’amata etangalijja

Obuzito obw’enjawulo/ g/cm3

ASTM D792

1.42

1.44

1.45

Obukaluba/olubalamaA

ASTM D2240 nga bwe kiri

40

50

60

Amaanyi g’okusika/MPa

ASTM D412

10.1

10.2

10.3

Okuwanvuwa Ku Luwummula /% .

ASTM D412

490

457

440

Amaanyi g’amaziga/KN/m

ASTM D624-B

35

42

43

Okunyigiriza Set(177°C * 22h)

ASTM D395

11

11

12

*Okuziyiza ebbugumu
225°C×72h

Enkyukakyuka y’obukaluba /shore A

+3

+3

+2

Enkyukakyuka y’amaanyi g’okusika, % .

-19

-16

-17

Okuwanvuwa ku nkyukakyuka y’okuwummulamu, % .

-14

-17

-18

Amafuta C

Enkyukakyuka mu ddoboozi/%

23°C/essaawa 72

ASTM D471

23

21

20

Embeera y’okuwonya

0.7 DBPH, Okuwonya press: 170°C×15min,Oluvannyuma lw’okuwonya: 200°C×4h


Ebikolwa ebisemba:


Kiteesebwako okukozesa ekitundu 0.6 ku 1 eky’ekirungo ky’eddagala lya bisdipenta okukola vulcanization (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).


Bakasitoma balina okulonda ebbugumu n’obudde obusinga okutuukirawo okuwonya okusinziira ku bunene bw’ekintu n’engeri y’okuwonya.


Okupakinga ebintu:


Ekintu kino si kya bulabe, mu kifo ky’ekyo kikoleddwa mu kaadi, obuveera, ne kkiro 10 buli nsawo, ensawo 2 buli bbokisi.


Emyaka gy’okutereka:


Ekintu kino kirina obusobozi bw’okukulukuta mu nnyonta, ensawo erina okwewalibwa okusobola obutaba nga eyonoonese nga bagitambuza oba nga bagikozesa.


Kuuma mu mbeera ennyogovu era enkalu ng’owangaala emyezi 12.

Jjuuzi: 
Ekiddako: 

ENKOZESA Y'AMAWANGA

EBINTU EBYAFFE

AMAWULIRE AG'OKUKWATAGANA

Add: No.33, Lane 159, Oluguudo lwa Taiye, Disitulikiti y’e Fengx, Shanghai
Essimu / WhatsApp / Skype: +86 15221953351 ku ssimu
Eddembe ly’okuwandiika     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap . |   Enkola y'Ebyama | Obuwagizi bwa . Leadong ..