FV9200
Herchy
| ~!phoenix_var111_3!~ | |
|---|---|
| ~!phoenix_var111_4!~ | |
barang |
Indikator |
|||
biji |
FV9240 |
FV9250 |
FV9260 |
|
Cara Tes / Penampilan |
Tembus putih susu |
|||
Gravitasi spesifik / g / cm3 |
ASTM D792 |
1.42 |
1.44 |
1.45 |
Kekerasan / pantaiA |
ASTM D2240 |
40 |
50 |
60 |
Kekuatan Tarik/MPa |
ASTM D412 |
10.1 |
10.2 |
10.3 |
Elongation ing Break /% |
ASTM D412 |
490 |
457 |
440 |
Kekuwatan luh/KN/m |
ASTM D624-B |
35 |
42 |
43 |
Set Kompresi (177 ℃ * 22h) |
ASTM D395 |
11 |
11 |
12 |
* Tahan Panas |
Owah-owahan kekerasan / pantai A |
+3 |
+3 |
+2 |
owah-owahan kekuatan tarik,% |
-19 |
-16 |
-17 |
|
Elongasi ing owah-owahan break,% |
-14 |
-17 |
-18 |
|
Bahan bakar C Ganti Volume/% 23 ℃ / 72 jam |
ASTM D471 |
23 |
21 |
20 |
Kondisi Curing |
0,7 DBPH, Press cure: 170 ℃ × 15 menit, Post cure: 200 ℃ × 4h |
|||
Tindakan sing disaranake:
Disaranake nggunakake 0,6 nganti 1 bagean agen kimia bisdipenta kanggo vulkanisasi (2,5-dimetil-2,5-bis(tert-butylperoxy)heksana).
Pelanggan kudu milih suhu lan wektu sing paling cocok kanggo ngobati adhedhasar ukuran produk lan cara ngobati.
Kemasan produk:
Produk iki ora mbebayani, nanging kasusun saka karton, plastik, lan 10 kilogram saben tas, 2 tas saben kothak.
Umur panyimpenan:
Produk iki nduweni kapasitas aliran kadhemen, tas kudu nyingkiri supaya ora rusak nalika transportasi utawa panggunaan.
Simpen ing lingkungan sing adhem lan garing kanthi umur simpan 12 wulan.