Hydrogenated Nitrile Rubber Precompound And Compound-HNBR

Hydrogenated nitrile rubber (HNBR or HSN) is the product of hydrogenation and saturation of the carbon-carbon double bond in the molecular chain of nitrile rubber, so it is also called highly saturated nitrile rubber.
Availability:
Quantity:

Hydrogenated nitrile rubber precompound and compound-HNBR


Hydrogenated nitrile rubber (HNBR or HSN) is the product of hydrogenation and saturation of the carbon-carbon double bond in the molecular chain of nitrile rubber, so it is also called highly saturated nitrile rubber.


HNBR has good oil resistance (good resistance to fuel oil, lubricants, aromatic solvents); and due to its highly saturated structure, it has good heat resistance, excellent chemical resistance (good resistance to Freon, acids and alkalis), excellent ozone resistance, and high resistance to permanent deformation in compression; at the same time, HNBR also has high strength, high tearing performance. HNBR also has high strength, high tear performance, excellent wear resistance, etc. It is one of the rubber with excellent overall performance.


Herchy Rubber has a professional technical team with rich experience in HNBR R&D. We can develop products for different applications according to customers' needs. And enjoy high reputation in China and the world.


HerchyVulcanization typeAcrylonitrile contentMooney viscosityHardnessTensile strengthElongation at breakIRM 903 Volume changeCompression setApplicationCharacter






150℃*72h150℃*72h ASTM D395 Type B
Grade%ML(1+4)100℃Shore AMpa%%%
HNBR-S6035Sulfur3550~1006017~24300~500<20<60Products in oilfield industry,Great elongation,
Good self-adhesiveness,
Exllent processing
HNBR-S7035Sulfur3550~1007017~24300~500<20<60Products in oilfield industry,
Automobile industry,
Belt
Dynamic fatigue resistance ,
Good self-Resistance,
Exllent processing
HNBR-S8035Sulfur3550~1008017~24300~500<20<60Drilling pipe protective layers,
Ppressure accumulators
High pressure resistance,
Good self-adhesiveness
HNBR-S6043Sulfur4350~1006017~24300~500<10<60Automobile fuel,
Products in oilfield industry
Oil resistance,
Exllent processing
HNBR-S7043Sulfur4350~1007017~24300~500<10<60Products in oilfield industry,
Automobile industry,
Oil resistance,
Dynamic fatigue resistance ,
Good self-Resistance
HNBR-S8043Sulfur4350~1008017~24300~500<10<60Drilling pipe protective layers,
Ppressure accumulators
Oil resistance,
High pressure resistance,
Good self-adhesiveness
HNBR-P6035Peroxide3550~1006017~24200~350<20<30Automobile industry,
Aircraft manufacturing industry
High tempreture resistance,
Exllent processing
HNBR-P7035Peroxide3550~1007017~24200~350<20<30Construction industry,
Engine gaskets,
O-rings,
Seals
High tempreture resistance,
Good compression set
HNBR-P8035Peroxide3550~1008017~24200~350<20<30Drilling pipes,
Pressure accumulators,
High pressure resistance,
High tempreture resistance
HNBR-P6043Peroxide4350~1006017~24200~350<10<30Automobile fuel and Lubrication systemsOil resistance,
Exllent processing,
Good compression set
HNBR-P7043Peroxide4350~1007017~24200~350<10<30Engine gaskets,
O-rings,
Seals,
Belt
Oil resistance,
Good compression set,
Exllent processing
HNBR-P8043Peroxide4350~1008017~24200~350<10<30Drilling pipes,
Pressure accumulators
Oil resistance,
High pressure resistance,
High tempreture resistance


1. Triangular belt

2. Vibration Isolators

3. Seals

4. Heat resistant pipe

5. Drilling protection box

6. Pistons for mud pumps

7. Sealing gaskets for the automotive industry

8. Seals for power stations

9. Hydraulic hoses

10. Hydraulic seals

11. Cable sheaths for power stations

12. Printing and fabric rollers

13. Seals for aerospace

14. Coverings

15.Fuel bladders


Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.