FV9600 Fluorosilikon

Prodhuk iki nduweni retardasi api sing apik, ketemu tingkat tahan api UL94/FV 0. resistance lenga banget, resistance solvent, resistance suhu dhuwur lan kurang
  • FV9600

  • Herchy

Kasedhiyan:
Jumlah:

Indikator teknis

barang

Indeks

sasmita

FV9660

FV9670

Penampilan

Metode Tes

Putih

Gravitasi spesifik/g/cm3

ASTM D792

1.46

1.48

Kekerasan / pantaiA

ASTM D2240

60

70

Kekuatan Tarik/MPa

ASTM D412

6.8

6.5

Elongation ing Break /%

ASTM D412

310

290

Kekuwatan luh/KN/m

ASTM D624-B

17

17

* Tahan Panas
200 ℃ × 72h

Owah-owahan kekerasan / pantai A

+5

+5

owah-owahan kekuatan tarik,%

3.8

3.5

owah-owahan kekuatan tarik,%

161

154

IRM903
Volume Ganti/%
150 ℃ / 72h

ASTM D471

5.5

5.2

Bahan bakar C
Laju owah-owahan volumetrik/%
23℃/72h

ASTM D471

20

20

Tingkat Flame-retardant

GBT10707-2008

FV 0

FV 0

Kondisi Curing

Tambah 0,7 bagean bis (2 + 5), siji tahap vulkanisasi 170 ℃ × 15min, rong tahap vulkanisasi: 200 ℃ × 4h.


Rekomendasi pangolahan


Gunakake 0,6 nganti 1 bagean agen vulkanisir bis-dipenta(2,5-dimetil-2,5-bis(tert-butylperoxy)heksana).

Suhu ngobati lan wektu ditemtokake miturut ukuran produk lan cara ngobati sing ditindakake dening pelanggan.

Kemasan Produk


Produk iki yaiku Barang Non-mbebayani, kemasan karton, kemasan njero kantong plastik, sepuluh kilogram saben tas, rong tas saben kothak.

Periode Panyimpenan


Amarga produk iki nduweni sifat aliran kadhemen, sajrone transportasi lan digunakake, tas kudu dihindari supaya rusak.

Simpen ing papan sing adhem lan garing, umur simpan 12 wulan.

Sadurunge: 
Sabanjure: 

LINKS CEPAT

PRODUK KAMI

INFORMASI KONTAK

Tambah: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telpon / WhatsApp / Skype: +86 15221953351
Hak Cipta     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Kebijakan Privasi | Dhukungan dening Leadong.