Zinc oxide bụ ihe inorganic nwere usoro kemịkalụ ZnO, oxide nke zinc. Ọ na-esighi ike na mmiri na soluble na acid na ntọala siri ike. Zinc oxide bụ ihe mgbakwunye kemịkalụ na-ejikarị eme ihe na rọba sịntetịt.
Ọdịdị: White na-acha odo odo ntụ ntụ
Znic oxide ọdịnaya: 88-93%
metal dị arọ dị ka Pb2 + (%): 0.001 Max.
Ọla kọpa dị ka Cu2+ (%): 0.0005 Max.
Manganese dị ka Mn2+ (%): 0.001 Max.
Njupụta (g/mm3): 4.6
Specific elu mpaghara (m2/g): 40
Ọdịdị: Ọcha na-acha odo odo ntụ ntụ
Znic oxide Ọdịnaya: min 90%
Igwe dị arọ dị ka Pb2 + (%): 0.001 Max.
Ọla kọpa dị ka Cu2+ (%): 0.0005 Max.
Manganese dị ka Mn2+ (%): 0.001 Max.
Njupụta (g/mm3): 3.6
Specific elu mpaghara (m2/g): 40
Ọdịdị: Ọcha na-acha odo odo ntụ ntụ
Znic oxide ọdịnaya: min 40%
metal dị arọ dị ka Pb2 + (%): 0.002 Max.
Ọla kọpa dị ka Cu2+ (%): 0.001 Max.
Manganese dị ka Mn2+ (%): 0.001 Max.