Ethylene Propylene Rubber – EPDM/EPM
Isi uru arụmọrụ EPDM bụ ndị a.
(1) arụmọrụ dị elu, yana njupụta rọba raw nke naanị 0.86-0.90g / cm3, nke bụ rọba nkịtị kachasị mfe na njupụta roba raw; na enwere ike itinye ya na karama buru ibu iji belata ọnụ ahịa rọba.
(2) Mgbochi ịka nká nke ọma, nguzogide ihu igwe, nkwụsị ozone, nkwụsi ike nke ìhè anyanwụ, nkwụsị ọkụ, mmiri na-eguzogide mmiri, mmiri na-eguzogide mmiri, nkwụsị nke UV, nguzogide radieshon na ihe ndị ọzọ ịka nká. Mgbe a na-eji EPDM jikọtara ya na rubbers diene ndị ọzọ na-adịghị mma dị ka NR, SBR, BR, NBR, CR, wdg, ọ nwere ike rụọ ọrụ dị ka ihe mgbochi polymer ma ọ bụ onye na-egbochi ịka nká.
(3) Nguzogide kemịkalụ dị mma, acid, alkali, detergent, mmanụ anụmanụ na ihe oriri, mmanya, ketone, wdg; ezigbo mmiri na-eguzogide, mmiri na-ekpo ọkụ, mmiri na-eguzogide mmiri; pola mmanụ iguzogide.
(4) Ọmarịcha mkpuchi mkpuchi arụmọrụ, olu resistivity 1016Ω-cm, mmebi voltaji 30-40MV / m, dielectric mgbe niile (1kHz, 20 ℃) 2.27.
(5) Wide arụ ọrụ okpomọkụ nso, kacha nta arụ ọrụ okpomọkụ -40-60 ℃, nwere ike ji mee ogologo oge n'okpuru 130 ℃.
Hirsch Rubber na-ebupụ EPDM/EPM na mba 15 gụnyere United States, Russia, Brazil, Argentina, South Korea, Germany, Italy, Spain, Australia, na India.
Ethylene Propylene Rubber-EPDM/EPM
| Herchy | Mooney viscosity | Mooney viscosity | Mooney viscosity | Ọdịnaya Ethylene | Ọdịnaya ENB | Ọdịnaya ndọtị-mmanụ | Ngwa | agwa |
| Ọkwa |
ML (1+4)100℃ | ML (1+4) 125 ℃ | ML (1+4)150℃ | wt% | wt% | PHR | ||
| S501A | 44 | [30] | 53 | 4.1 | Ngwaahịa na-akpụzi injection; Ngwaahịa siri ike dị elu; | Viscosity Mooney dị ala; Ezi liquidity; Nguzogide okpomọkụ dị ala; |
||
| S505A | 45 | [29] | 55 | 9.4 | Ngwaahịa siri ike dị elu :Taya sidewall; Akụkụ foamed; | Viscosity Mooney dị ala; Ezi liquidity; Ọdịnaya ENB dị elu; Ọsọ ọgwụgwọ ngwa ngwa; Nguzogide okpomọkụ dị ala; |
||
| S537-3 | 35 | 57 | 2.3 | Ọkpụkpụ ime;Akpụkpọ ụkwụ; Akụkụ igwe eji arụ ọrụ | Nnukwu nguzogide okpomọkụ; |
|||
| S537-2 | 40 | 57 | 3 | N'ime tube; Akụkụ igwe ihe nrụpụta | Nnukwu nguzogide okpomọkụ; |
|||
| S512F | 63 | 69 | 4.5 | Hose;Oghere ụzọ na windo akara; Ngwaahịa Extrusion; | Ọdịnaya ethylene dị elu; Njirimara igwe dị elu; Ngwongwo nhazi mara mma |
|||
| S5890F | [87] | 64 | 68 | 5.5 | Hose;Oghere akara akara;Gasket; | Njuputa dị elu; Ngwongwo nhazi mara mma; |
||
| S552 | 84 | 58 | 4.1 | Hose; Oke akara akara; Gasket; Ngwaahịa ụlọ ọrụ; | Ngwongwo nhazi dị mma; obere okpomọkụ na-eguzogide; High n'ibu Njirimara |
|||
| S552-1 | 84 | 58 | 5.7 | Hose; Oke akara akara; Ngwaahịa ụlọ ọrụ; | Ngwongwo nhazi dị oke mma; Nguzogide okpomọkụ dị ala; Njirimara igwe dị elu; nnukwu nlọghachi |
|||
| S553 | [98] | 72 | 62 | 4.5 | Ọnụ ụzọ na windo akara; | High Mooney viscosity; Ndochi dị elu; Obere okpomọkụ na-eguzogide; Njirimara akụrụngwa dị elu; |
||
| S5206F | [84] | 81 | 60 | 8.5 | Profaịlụ sponge; Akụkụ ndị nwere ụfụfụ; | Viscosity Mooney dị elu; Ọdịnaya ENB dị elu; Ọsọ ọgwụgwọ ngwa ngwa; Njirimara akụrụngwa dị elu; |
||
| S5527F | [109] | 81 | 60 | 8.5 | Profaịlụ sponge; Akụkụ ndị na-afụ ụfụ;Ngwaahịa rebound dị elu; | Ndochi dị elu; High Mooney viscosity; Ọdịnaya ENB dị elu; Ọsọ ọgwụgwọ ngwa ngwa; akụrụngwa akụrụngwa dị elu; |
||
| S6090WF | 53 | 70 | 5.7 | 50 | Ngwaahịa siri ike dị ala;Hose;Akàrà ọnụ ụzọ igwe;Akụkụ waya ụgbọ ala;Elu rebound ngwaahịa;Elu n'ibu Njirimara | Ọdịnaya ethylene dị elu; elu Mooney viscosity; akụrụngwa akụrụngwa dị elu; ihe nhazi dị mma; |
||
| S600WF | 61 | [41] | 72 | 4 | 100 | Ngwaahịa siri ike dị ala;Taya igwe kwụ otu ebe, eriri waya ụgbọ ala | Ndochi dị elu; akụrụngwa akụrụngwa dị elu; Ngwongwo nhazi mara mma; |
|
| S7486F | 92 | 67 | 60 | 9 | Profaịlụ sponge; Oghere mkpuchi mkpuchi; Akụkụ foamed; | Ọdịnaya ethylene dị ala; Ọdịnaya ENB dị elu; Ọsọ ọsọ ọsọ; |
||
| S6075WF | 50 | 60 | 4.7 | 75 | Ngwaahịa siri ike dị ala; Ngwaahịa ịkpụzi injection ;Akụkụ waya ụgbọ ala ;Njiri arụ ọrụ dị elu | Ọdịnaya ethylene dị ala; High Mooney viscosity; Ngwongwo nhazi dị mma; obere okpomọkụ na-eguzogide; |
| Herchy | Mooney viscosity | Mooney viscosity | Mooney viscosity | Ọdịnaya Ethylene | Ọdịnaya ENB | Ọdịnaya ndọtị-mmanụ | Ngwa | agwa |
| Ọkwa | ML (1+4)100℃ | ML (1+4) 125 ℃ | ML (1+4)150℃ | wt% | wt% | PHR | ||
| J-2070 | 44* | 57.8 | 1.9 | Ọkpụkpụ ime;Akpụkpọ ụkwụ; Akụkụ igwe eji arụ ọrụ | Okpomọkụ na-eguzogide elu;Obere okpomọkụ na-eguzogide; | |||
| J-2080 | 53 | 62 | 2 | Ọkpụkpụ ime;Akpụkpọ ụkwụ; Akụkụ igwe eji arụ ọrụ | Nnukwu okpomọkụ na-eguzogide;Obere okpomọkụ eguzogide;Elu n'ibu Njirimara | |||
| 3062E | 41 | 68.5 | 3.9 | 20 | Ngwaahịa na-akpụzi injection ;Hose;Oghere ụzọ na windo akara; Ngwaahịa Extrusion; | Ọdịnaya ethylene dị elu; Njirimara igwe dị elu; Ngwongwo nhazi mara mma |
||
| J-3060P | 45 | 68.5 | 4 | Hose;Oghere ụzọ na windo akara; Ngwaahịa Extrusion; | Ọdịnaya ethylene dị elu; Njirimara igwe dị elu; Ngwongwo nhazi mara mma |
|||
| J-3080 | 70 | 68.5 | 4 | Hose;Oghere ụzọ na windo akara; Ngwaahịa Extrusion; | Ọdịnaya ethylene dị elu; Njirimara igwe dị elu; Ngwongwo nhazi mara mma |
|||
| J-3080P | 70 | 68.5 | 4 | Hose;Oghere ụzọ na windo akara; Ngwaahịa Extrusion; | Ọdịnaya ethylene dị elu; Njirimara igwe dị elu; Ngwongwo nhazi mara mma |
|||
| J-3092E | 60 | 57.2 | 4.6 | 20 | Hose;Oghere ụzọ na windo akara; Ngwaahịa Extrusion; | Ọdịnaya ethylene dị elu; Njirimara igwe dị elu; Ngwongwo nhazi mara mma |
||
| 4045 | 45 | 52 | 7.7 | Ngwaahịa siri ike dị elu :Taya sidewall; Akụkụ foamed; | Viscosity Mooney dị ala; Ezi liquidity; Ọdịnaya ENB dị elu; Ọsọ ọgwụgwọ ngwa ngwa; Nguzogide okpomọkụ dị ala; |
|||
| J-4090 | 65 | 52.5 | 7.7 | Akụkụ taya taya; Akụkụ ndị nwere ụfụfụ; | Ọdịnaya ENB dị elu; Ọsọ ọgwụgwọ ngwa ngwa; Nguzogide okpomọkụ dị ala; |
| Herchy | Mooney viscosity | Mooney viscosity | Mooney viscosity | Ọdịnaya Ethylene | Propylene ọdịnaya | Ọdịnaya ENB | Ọdịnaya ndọtị-mmanụ | Ngwa | agwa |
| Ọkwa |
ML (1+4)100℃ | ML (1+4) 125 ℃ | ML (1+4)150℃ | wt% | wt% | wt% | PHR | ||
| CO 033 | 30 | 72 | 28 | ||||||
| CO 034 | 44 | 72 | 28 | ||||||
| CO 038 | 60 | 72 | 28 | ||||||
| CO 043 | 33 | 55 | 45 | ||||||
| CO 054 | 44 | 59 | 41 | ||||||
| CO 058 | 80 | 60 | 52 | 48 | |||||
| CO 059 | 79 | 59 | 41 | ||||||
| TER 4033 | 30 | 70 | 25 | 5 | Ngwaahịa siri ike dị elu; Ngwaahịa na-akpụzi ọgwụ injection; Mpempe akara akara rọba ụgbọ ala | Viscosity Mooney dị ala; Ezi liquidity; Ọdịnaya ethylene dị elu; Njirimara igwe dị elu; Ngwongwo nhazi mara mma |
|||
| TER 4038EP | 60 | 68.6 | 27 | 4.4 | Hose;Oghere ụzọ na windo akara; Ngwaahịa Extrusion; | Ọdịnaya ethylene dị elu; Njirimara igwe dị elu; Ngwongwo nhazi mara mma |
|||
| TER 4039 | 77 | 68.6 | 27 | 4.4 | Hose;Oghere ụzọ na windo akara; Ngwaahịa Extrusion; | Ọdịnaya ethylene dị elu; Njirimara igwe dị elu; Ngwongwo nhazi mara mma |
|||
| TER 4044 | 44 | 61 | 35 | 4 | Ngwaahịa na-akpụzi injection; Ngwaahịa siri ike dị elu; | Viscosity Mooney dị ala; Ezi liquidity; Njirimara igwe dị elu; Ngwongwo nhazi mara mma |
|||
| TER 4047 | 55 | 55.5 | 40 | 4.5 | Ọkpụkpụ breeki, Ngwaahịa a kpụrụ akpụ, Gasket; Akụkụ igwe eji arụ ọrụ | Ọdịnaya ethylene dị ala; Ngwongwo nhazi mara mma; Obere okpomọkụ na-eguzogide |
|||
| TER 4049 | 76 | 55.5 | 40 | 4.5 | Hose; Oke akara akara; Gasket; Ngwaahịa ụlọ ọrụ; | Ọdịnaya ethylene dị ala; Njirimara igwe dị elu; Obere okpomọkụ na-eguzogide |
|||
| TER 4334 | 28 | 68.3 | 27 | 4.7 | 43 | Ngwaahịa siri ike dị elu; Ngwaahịa na-akpụzi injection; Ụgbọ ala rọba akara warara; Ngwaahịa ụlọ ọrụ | Viscosity Mooney dị ala; Ezi liquidity; Ọdịnaya ethylene dị elu; Njirimara igwe dị elu; Ngwongwo nhazi mara mma |
||
| TER 4436 | 43 | 66.5 | 28 | 5.5 | 67 | Akara ọnụ ụzọ igwe ịsa akwa; Ngwaahịa ụlọ ọrụ | Ngwongwo nhazi mara mma; Njirimara igwe dị elu; |
||
| TER 4437 | 57 | 63.5 | 32 | 4.5 | 67 | Akara ọnụ ụzọ igwe ịsa akwa; Ngwaahịa ụlọ ọrụ; | Ngwongwo nhazi mara mma; Njirimara igwe dị elu; Nnukwu okpomọkụ na-eguzogide; |
||
| TER 4535 | 32 | 64.6 | 32 | 3.4 | 100 | Akara ọnụ ụzọ igwe na-asa akwa; Ngwaahịa a kpụrụ akpụ; | Ọdịnaya ENB dị ala; Nnukwu okpomọkụ na-eguzogide; |
||
| TER 6148 | 65 | 53 | 40 | 7 | 18 | Akụkụ ndị nwere ụfụfụ; Profaịlụ sponge; Ngwaahịa a kpụrụ akpụ; | Ọdịnaya ethylene dị ala; Ọdịnaya ENB dị elu; Ọsọ ọgwụgwọ ngwa ngwa; Obere okpomọkụ na-eguzogide |
||
| TER 6235 | 33 | 60.6 | 32 | 7.4 | 30 | Ọkpụkpọ dị n'ime;Akpụkpọ ụkwụ; Akụkụ foamed; Profaịlụ sponge, ngwaahịa a kpụrụ akpụ | Viscosity Mooney dị ala; Ezi liquidity; Ọdịnaya ethylene dị elu; Njirimara igwe dị elu; Ngwongwo nhazi mara mma; Ọdịnaya ENB dị elu; Ọsọ ọgwụgwọ ngwa ngwa; |
||
| TER 6537 | 43 | 60 | 32 | 8 | 100 | Akụkụ ndị nwere ụfụfụ; Profaịlụ sponge ;Akàrà ọnụ ụzọ igwe na-asa akwa; Ngwaahịa a kpụrụ akpụ | Ọdịnaya ENB dị elu; Ọsọ ọgwụgwọ ngwa ngwa; |
||
| Ọnụahịa kasị elu nke TER9046 | 67 | 60.1 | 31 | 8.9 | Akụkụ foamed; Profaịlụ sponge; Ngwaahịa ụlọ ọrụ | Ọdịnaya ENB dị elu; Ọsọ ọgwụgwọ ngwa ngwa; |
|||
| TER 4548 | 47 | 59.5 | 36 | 4.5 | 10 | Ọkpụkpọ dị n'ime; Akpụkpọ ụkwụ; Ngwaahịa a kpụrụ akpụ; Ngwaahịa ụlọ ọrụ; Ngwaahịa akpụziri | Viscosity Mooney dị ala; Ezi liquidity; |
||
| TER 8148 | 68 | 52.5 | 39 | 8.5 | 21 | Akụkụ foamed; Profaịlụ sponge; Ngwaahịa ụlọ ọrụ; Ngwaahịa akpụziri | Ọdịnaya ethylene dị ala; Ọdịnaya ENB dị elu; Ọsọ ọgwụgwọ ngwa ngwa; Obere okpomọkụ na-eguzogide |
||
| TER 7040 | 87 | 53.5 | 40 | 6.5 | Hose;Oghere ụzọ na windo akara; Ngwaahịa Extrusion; | Ọdịnaya ethylene dị ala; Akwa njuputa; elu Mooney viscosity; Njirimara igwe dị elu; Obere okpomọkụ na-eguzogide |
|||
| TER 4049 | 76 | 55.5 | 40 | 4.5 | Hose;Oghere ụzọ na windo akara; Ngwaahịa Extrusion; | Ọdịnaya ethylene dị ala; Obere okpomọkụ na-eguzogide |
|||
| TER 5029 | 80 | 69.5 | 25 | 5.5 | Hose;Oghere ụzọ na windo akara; Ngwaahịa Extrusion; | Akwa njuputa; Ọdịnaya ethylene dị elu; elu Mooney viscosity; Njirimara igwe dị elu |
1. Automotive akara warara
Ihe mkpuchi mkpuchi maka mkpuchi
Ọnụ ụzọ akara
Ihuenyo windo
Imechi mkpuchi mkpuchi anwụ
Akara ụgbọ ala
Mgbochi uzuzu
Glassrun ọwa
Mgbochi mkpọtụ
2. Hose
Ọkpụkpụ breeki
Igwe ọkụ ọkụ ọkụ akpaaka
Ọkụ na-ekpochapụ Skylight
3. Waya na eriri
Igwe ọkụ
Igwe mkpuchi rọba
eriri mpaghara
Igwe onyonyo
eriri akụrụngwa
4. Igwe anaghị agba nchara
Igwe mmiri anaghị egbochi mgbidi
Igwe mmiri anaghị ekpuchi elu ụlọ
Akwụkwọ mpịakọta mmiri na-adịghị na okporo ụzọ
Igwe mmiri anaghị egbochi mmiri ọwara
5. Taya
N'ime tube
Akụkụ taya
taya igwe kwụ otu ebe
6. Nkịtị kpụrụ ngwaahịa
Ihe mgbochi roba
Ute roba
Gasket
breeki nnukwu efere
7. Mgbanwe mmanụ na ubi ndị ọzọ
mmanu mmako