FV9600 Fluorosilicon

Ngwaahịa a nwere ezigbo ire ere, zute ọkwa UL94/FV 0 ire ere. Mmanya na-eguzogide mma, ihe mgbaze, elu na obere okpomọkụ na-eguzogide
  • FV9600

  • Herchy

Nnweta:
Ọnụ ọgụgụ:

Ngosipụta teknụzụ

Ihe

Index

Ọkwa

FV9660

FV9670

Ọdịdị

Ụzọ ule

Ọcha

Specific ike ndọda/g/cm3

ASTM D792

1.46

1.48

Isi ike/ikpere mmiriA

ASTM D2240

60

70

Ike tensile/MPa

ASTM D412

6.8

6.5

Nkwalite na ezumike /%

ASTM D412

310

290

Ike akwa/KN/m

ASTM D624-B

17

17

* Okpomọkụ Nguzogide
200 ℃ × 72h

Mgbanwe ike ike / osimiri A

+5

+5

Mgbanwe ike tensile,%

3.8

3.5

Mgbanwe ike tensile,%

161

154

IRM903 /%
Mgbanwe olu
150℃/72h

ASTM D471

5.5

5.2

Mmanụ ụgbọala C
Ọnụego mgbanwe/%
23℃/72h

ASTM D471

20

20

Ọkwa na-egbochi ire ọkụ

GBT10707-2008

FV 0

FV 0

Ọnọdụ ọgwụgwọ

Tinye 0.7 akụkụ nke bis(2+5), otu ogbo vulcanisation 170℃×15min, abụọ ogbo vulcanisation: 200℃×4h.


Ntuziaka nhazi Jiri


0.6 ruo 1 akụkụ bis-dipenta vulcanising agent (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).

A na-ekpebi okpomọkụ ọgwụgwọ na oge dịka nha ngwaahịa ahụ si dị na usoro ọgwụgwọ nke onye ahịa na-eme.

Nkwakọ ngwaahịa ngwaahịa


a bụ ngwaahịa na-adịghị ize ndụ, nkwakọ ngwaahịa katọn, nkwakọ ngwaahịa dị n'ime, kilogram iri kwa akpa, akpa abụọ n'otu igbe.

Oge nchekwa


Ebe ọ bụ na ngwaahịa a nwere ihe eji ebugharị oyi, n'oge njem na n'iji akpa ahụ kwesịrị izere agbaji.

Chekwaa n'ebe dị mma, ebe akọrọ ndụ ndụ ọnwa 12.

Nke gara aga: 
Osote: 

Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nwebiisinka     2023 Shanghai Herchy Rubber Co., Ltd. map saịtị |   Amụma nzuzo | Nkwado Site Leadong.