GA-2610 ƒe agbalẽ
Herchy ƒe ŋkɔ
| Nusiwo Li: | |
|---|---|
| Agbɔsɔsɔ: | |
Dodokpɔ: A/B ƒe xexlẽme si nye 1 :1, 130°C x 5min x 15MPa
| Nusiwo wowɔ ƒe nɔnɔmewo | |||||||||
| Nu si wowɔ | GA-2610 ƒe agbalẽ | GA-2620 ƒe agbalẽ | GA-2630 ƒe agbalẽa | GA-2640 ƒe agbalẽ | GA-2650 ƒe agbalẽa | GA-2660 ƒe agbalẽa | GA-2670 ƒe agbalẽa | GA-2680 ƒe agbalẽ | |
| Dzedzeme | Si me kɔ | ||||||||
| Viscosity(Pa.s) ƒe ʋeʋẽ lilili . |
1500 | 2000 | 2500 | 3000 | 3500 | 4000 |
4000 |
5500 |
|
| Sesẽme (ƑutaA) . | 10 | 20 | 30 | 40 | 50 |
60 |
70 |
80 |
|
| Eƒe kpekpeme(g/cm3) . | 1.08 | 1.10 | 1.10 | 1.11 | 1.12 |
1.13 |
1.14 |
1.15 |
|
| Ŋusẽ si wotsɔna ƒoa nu (MPa) . | 4.5 |
6.5 |
7.5 |
9.5 |
10.0 |
10.0 |
9.5 |
9.0 |
|
| Elongation(%) ƒe didime . | 900 | 880 | 800 | 700 | 550 |
450 |
350 |
350 |
|
| Aɖatsi ƒe ŋusẽ (kN/m) . | 8 | 12 | 15 | 25 | 35 |
35 |
30 |
30 |
|
| Linearshrinkage(%) ƒe ʋuʋu le fli me. | 2.3 | 2.1 | 2.1 | 2.1 | 2.0 |
2.0 |
2.0 |
2.0 |
|
| Gbeƒãɖeɖe(%) . | 90 |
90 | 90 | 90 | 90 | 90 | 90 | 90 | |