Ethylene Propylene ƒe rababa – EPDM/EPM
EPDM ƒe dɔwɔwɔ ƒe viɖe veviwoe nye esiawo.
(1) Gazazã gã ƒe dɔwɔwɔ, kple rababa ƒuƒu ƒe kpekpeme si nye 0.86-0.90g/cm3 ko, si nye rababa bɔbɔetɔ si le bɔbɔe wu si me rababa ƒuƒu ƒe kpekpeme le; eye woate ŋu atsɔe ade atukpa me le agbɔsɔsɔ gã me be wòaɖe rababa ƒe asi dzi akpɔtɔ.
(2) Tsitsi ƒe tsitretsitsi nyuie, yame ƒe nɔnɔme ƒe tsitretsitsi, ozone ƒe tsitretsitsi, ɣe ƒe keklẽ ƒe tsitretsitsi, dzoxɔxɔ ƒe tsitretsitsi, tsi ƒe tsitretsitsi, tsi ƒe dzoxɔxɔ ƒe tsitretsitsi, UV ƒe tsitretsitsi, keklẽŋusẽ ƒe tsitretsitsi kple tsitsi ƒe nɔnɔme bubuwo. Ne wozã EPDM kpe ɖe diene rababa bubu siwo me mekɔ o abe NR, SBR, BR, NBR, CR, kple bubuawo ene ŋu la, ate ŋu awɔ dɔ abe polymer antioxidant alo anti-aging agent ene.
(3) Atikewo ƒe tsitretsitsi nyuie, acid, alkali, atike si wotsɔna klɔa nu, lãwo kple amagbewo ƒe ami, aha, ketone, kple bubuawo; tsi ƒe tsitretsitsi nyuie, tsi si xɔ dzo akpa, tsi ƒe dzoxɔxɔ ƒe tsitretsitsi; polar ami ƒe tsitretsitsi.
(4) Excellent insulation dɔwɔwɔ, gbeɖiɖi ƒe tsitretsitsi 1016Ω-cm, gbagbã voltage 30-40MV / m, dielectric madzudzɔmadzudzɔe (1kHz, 20 ° C) 2.27.
(5) Woate ŋu azã dzoxɔxɔ si keke ta le dɔwɔwɔ me, dzoxɔxɔ si le dɔ wɔm suetɔ kekeake -40-60°C, ate ŋu azã ɣeyiɣi didi aɖe le 130°C te.
Hirsch Rubber ɖoa EPDM/EPM ɖe dukɔ 15 siwo dometɔ aɖewoe nye United States, Russia, Brazil, Argentina, South Korea, Germany, Italy, Spain, Australia, kple India.
Ethylene Propylene ƒe rababa-EPDM/EPM
| Herchy ƒe ame | Mooney ƒe ʋeʋẽ lilili | Mooney ƒe ʋeʋẽ lilili | Mooney ƒe ʋeʋẽ lilili | Ethylene si le eme | ENB Emenyawo | Extend-oil Nusiwo le eme | Mᴐbibia | Nᴐnᴐme |
| Ɖoƒe |
ML (1+4) 100°C ƒe didime | ML (1+4) 125°C ƒe dzoxɔxɔ | ML (1+4) 150°C ƒe didime | wt% . | wt% . | PHR | ||
| S501A ƒe ŋkɔ | 44 | [30] . | 53 | 4.1 | Injection Molding Products ;High sesẽnuawo; | Mooney ƒe ʋeʋẽ si bɔbɔ; Gazazã nyuie; Dzoxɔxɔ si bɔbɔ ƒe tsitretsitsi; |
||
| S505A | 45 | [29] . | 55 | 9.4 | High hardness products;Taya ƒe axadzigli;Foamed akpawo; | Mooney ƒe ʋeʋẽ si bɔbɔ; Gazazã nyuie; ENB ƒe agbɔsɔsɔ si sɔ gbɔ; Dɔyɔyɔ kabakaba; Dzoxɔxɔ si bɔbɔ ƒe tsitretsitsi; |
||
| S537-3 ƒe agbalẽ | 35 | 57 | 2.3 | Ememe tube;Afɔkpa;Xɔtumɔ̃wo ƒe akpa aɖewo | Dzoxɔxɔ gã ƒe tsitretsitsi; Dzoxɔxɔ ƒe tsitretsitsi si bɔbɔ; |
|||
| S537-2 | 40 | 57 | 3 | Inner tube;Xɔtumɔ̃wo ƒe akpa aɖewo | Dzoxɔxɔ gã ƒe tsitretsitsi; Dzoxɔxɔ ƒe tsitretsitsi si bɔbɔ; |
|||
| S512F ƒe agbalẽ | 63 | 69 | 4.5 | Hose;Ʋɔtru kple fesre nutrenu strips;Extrusion Product; | Ethylene si sɔ gbɔ ɖe eme; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake |
|||
| S5890F ƒe agbalẽ | [87] . | 64 | 68 | 5.5 | Hose;Dense nutrenu strip;Gasket; | Kɔkɔe yɔyɔ; Enyo ŋutɔ dɔwɔwɔ ƒe nunɔamesi; |
||
| S552 | 84 | 58 | 4.1 | Hose;Dense nutrenu strip;Gasket;Dɔwɔƒewo ƒe nuwɔna; | Dɔwɔwɔ nyuie ƒe nɔnɔme; Dzoxɔxɔ ƒe tsitretsitsi si bɔbɔ; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔ |
|||
| S552-1 | 84 | 58 | 5.7 | Hose;Dense nutrenu strip;Dɔwɔƒewo ƒe nuwɔna; | Dɔwɔwɔ ƒe nɔnɔme nyuitɔ kekeake; Dzoxɔxɔ ƒe tsitretsitsi si bɔbɔ; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔ; Gbugbɔgadzɔ gã |
|||
| S553 | [98] . | 72 | 62 | 4.5 | Ʋɔtru kple fesre nutrenu strips;Tsi mate ŋu age ɖe eme o; | Mooney viscosity kɔkɔ; Filling kɔkɔ; Dzoxɔxɔ ƒe tsitretsitsi sue; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔ; |
||
| S5206F ƒe agbalẽ | [84] . | 81 | 60 | 8.5 | Sponge profile;Akpa siwo me fu le; | Mooney ƒe ʋeʋẽ lilili; ENB ƒe agbɔsɔsɔ gã; Dɔyɔ kabakaba; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔ; |
||
| S5527F ƒe agbalẽ | [109] . | 81 | 60 | 8.5 | Sponge profile;Foamed akpawo;High rebound nuwɔna; | Kɔkɔe yɔyɔ; Mooney viscosity kɔkɔ; ENB ƒe agbɔsɔsɔ gã; Dɔyɔ kabakaba; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔ; |
||
| S6090WF ƒe agbalẽ | 53 | 70 | 5.7 | 50 | Low hardness products;Hose;Klɔmɔ̃ ƒe ʋɔtru nutrenuwo;Ʋu ka harness;High rebound nu;High mɔ̃ɖaŋu nɔnɔmewo | Ethylene si sɔ gbɔ; Moone ƒe ʋeʋẽ lilili; Mɔ̃ɖaŋununya ƒe nɔnɔme gãwo; Dɔwɔwɔ ƒe nɔnɔme nyui aɖe; |
||
| S600WF ƒe agbalẽ | 61 | [41] . | 72 | 4 | 100 | Low hardness products;Keke taya;Ʋu ka harness;High rebound nuwɔna;High mɔ̃ɖaŋu nɔnɔmewo | Kɔkɔe ; yɔyɔ |
|
| S7486F ƒe nyawo | 92 | 67 | 60 | 9 | Sponge profile;Dense nutrenu strip;Foamed akpawo; | Ethylene ƒe agbɔsɔsɔ si le sue; ENB ƒe agbɔsɔsɔ fũ; Dɔyɔ kabakaba; |
||
| S6075WF ƒe agbalẽ | 50 | 60 | 4.7 | 75 | Low hardness products;Injection Molding Products ;Ʋu ka harness;Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo | Ethylene ƒe agbɔsɔsɔ si le sue; Moone ƒe ʋeʋẽ lilili; Dɔwɔwɔ ƒe nɔnɔme nyui aɖe; Dzoxɔxɔ ƒe tsitretsitsi si bɔbɔ; |
| Herchy ƒe ame | Mooney ƒe ʋeʋẽ lilili | Mooney ƒe ʋeʋẽ lilili | Mooney ƒe ʋeʋẽ lilili | Ethylene si le eme | ENB Emenyawo | Extend-oil Nusiwo le eme | Mᴐbibia | Nᴐnᴐme |
| Ɖoƒe | ML (1+4) 100°C ƒe didime | ML (1+4) 125°C ƒe dzoxɔxɔ | ML (1+4) 150°C ƒe didime | wt% . | wt% . | PHR | ||
| J-2070 ƒe agbalẽ | 44* . | 57.8 | 1.9 | Ememe tube;Afɔkpa;Xɔtumɔ̃wo ƒe akpa aɖewo | Dzoxɔxɔ kɔkɔ ƒe tsitretsitsi;Low dzoxɔxɔ ƒe tsitretsitsi; | |||
| J-2080 ƒe agbalẽ | 53 | 62 | 2 | Ememe tube;Afɔkpa;Xɔtumɔ̃wo ƒe akpa aɖewo | Dzoxɔxɔ kɔkɔ ƒe tsitretsitsi;Dzoxɔxɔ ƒe tsitretsitsi bɔbɔe;Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo | |||
| 3062E | 41 | 68.5 | 3.9 | 20 | Injection Molding Products ;Hose;Ʋɔtru kple fesre nutrenu strips;Extrusion Product; | Ethylene si sɔ gbɔ ɖe eme; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake |
||
| J-3060P | 45 | 68.5 | 4 | Hose;Ʋɔtru kple fesre nutrenu strips;Extrusion Product; | Ethylene si sɔ gbɔ ɖe eme; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake |
|||
| J-3080 ƒe agbalẽ | 70 | 68.5 | 4 | Hose;Ʋɔtru kple fesre nutrenu strips;Extrusion Product; | Ethylene si sɔ gbɔ ɖe eme; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake |
|||
| J-3080P | 70 | 68.5 | 4 | Hose;Ʋɔtru kple fesre nutrenu strips;Extrusion Product; | Ethylene si sɔ gbɔ ɖe eme; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake |
|||
| J-3092E ƒe agbalẽ | 60 | 57.2 | 4.6 | 20 | Hose;Ʋɔtru kple fesre nutrenu strips;Extrusion Product; | Ethylene si sɔ gbɔ ɖe eme; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake |
||
| 4045 | 45 | 52 | 7.7 | High hardness products;Taya ƒe axadzigli;Foamed akpawo; | Mooney ƒe ʋeʋẽ si bɔbɔ; Gazazã nyuie; ENB ƒe agbɔsɔsɔ si sɔ gbɔ; Dɔyɔyɔ kabakaba; Dzoxɔxɔ si bɔbɔ ƒe tsitretsitsi; |
|||
| J-4090 ƒe agbalẽ | 65 | 52.5 | 7.7 | Taya ƒe axadzigli;Akpa siwo me fu le; | ENB ƒe agbɔsɔsɔ si sɔ gbɔ; Dɔyɔyɔ kabakaba; Dzoxɔxɔ si bɔbɔ ƒe tsitretsitsi; |
| Herchy ƒe ame | Mooney ƒe ʋeʋẽ lilili | Mooney ƒe ʋeʋẽ lilili | Mooney ƒe ʋeʋẽ lilili | Ethylene si le eme | Propylene si le eme | ENB Emenyawo | Extend-oil Nusiwo le eme | Mᴐbibia | Nᴐnᴐme |
| Ɖoƒe |
ML (1+4) 100°C ƒe didime | ML (1+4) 125°C ƒe dzoxɔxɔ | ML (1+4) 150°C ƒe didime | wt% . | wt% . | wt% . | PHR | ||
| CO 033 ƒe xexlẽme | 30 | 72 | 28 | ||||||
| CO 034 ƒe xexlẽme | 44 | 72 | 28 | ||||||
| CO 038 ƒe xexlẽme | 60 | 72 | 28 | ||||||
| CO 043 ƒe xexlẽme | 33 | 55 | 45 | ||||||
| CO 054 ƒe xexlẽme | 44 | 59 | 41 | ||||||
| CO 058 ƒe xexlẽme | 80 | 60 | 52 | 48 | |||||
| CO 059 ƒe xexlẽme | 79 | 59 | 41 | ||||||
| TER 4033 ƒe xexlẽdzesi | 30 | 70 | 25 | 5 | Kɔkɔ sesẽ nuawo;Injection Molding Nuwo;Ʋu rababa nutrenu strip | Mooney ƒe ʋeʋẽ si bɔbɔ; Gazazã nyuie; Ethylene si sɔ gbɔ ɖe eme; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake |
|||
| TER 4038EP ƒe xexlẽdzesi | 60 | 68.6 | 27 | 4.4 | Hose;Ʋɔtru kple fesre nutrenu strips;Extrusion Product; | Ethylene si sɔ gbɔ ɖe eme; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake |
|||
| TER 4039 ƒe xexlẽdzesi | 77 | 68.6 | 27 | 4.4 | Hose;Ʋɔtru kple fesre nutrenu strips;Extrusion Product; | Ethylene si sɔ gbɔ ɖe eme; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake |
|||
| TER 4044 ƒe xexlẽdzesi | 44 | 61 | 35 | 4 | Injection Molding Products ;High sesẽnuawo; | Mooney ƒe ʋeʋẽ si bɔbɔ; Gazazã nyuie; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake |
|||
| TER 4047 ƒe xexlẽdzesi | 55 | 55.5 | 40 | 4.5 | Brek Hose;Molded nuwɔna ;Gasket;Xɔtumɔ̃wo ƒe akpa aɖewo;Ememe tube;Afɔkpa; | Ethylene si mesɔ gbɔ o; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake; Dzoxɔxɔ ƒe tsitretsitsi si bɔbɔ |
|||
| TER 4049 ƒe xexlẽdzesi | 76 | 55.5 | 40 | 4.5 | Hose;Dense nutrenu strip;Gasket;Dɔwɔƒewo ƒe nuwɔna; | Ethylene si mesɔ gbɔ o; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dzoxɔxɔ ƒe tsitretsitsi si bɔbɔ |
|||
| TER 4334 ƒe xexlẽdzesi | 28 | 68.3 | 27 | 4.7 | 43 | High hardness products;Injection Molding Products;Ʋu rababa nutrenu strip;Dɔwɔƒewo ƒe nuwɔna | Mooney ƒe ʋeʋẽ si bɔbɔ; Gazazã nyuie; Ethylene si sɔ gbɔ ɖe eme; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake |
||
| TER 4436 ƒe xexlẽdzesi | 43 | 66.5 | 28 | 5.5 | 67 | Nufamɔ̃ ƒe ʋɔtru nutrenuwo;Dɔwɔƒewo ƒe nuwɔna | Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; |
||
| TER 4437 ƒe xexlẽdzesi | 57 | 63.5 | 32 | 4.5 | 67 | Nufamɔ̃ ƒe ʋɔtru nutrenuwo;Dɔwɔƒewo ƒe nuwɔna; | Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dzoxɔxɔ si nu sẽ ƒe tsitretsitsi; |
||
| TER 4535 ƒe xexlẽdzesi | 32 | 64.6 | 32 | 3.4 | 100 | Nufamɔ̃ ƒe ʋɔtru nutrenuwo;Molded products ; | ENB ƒe agbɔsɔsɔ si le ʋɛ; Dzoxɔxɔ si nu sẽ ƒe tsitretsitsi; |
||
| TER 6148 ƒe xexlẽdzesi | 65 | 53 | 40 | 7 | 18 | Foamed akpawo;Sponge profile;Molded nusiwo wowɔ ; | Ethylene si mesɔ gbɔ o; ENB ƒe agbɔsɔsɔ si sɔ gbɔ; Dɔyɔyɔ kabakaba; Dzoxɔxɔ ƒe tsitretsitsi si bɔbɔ |
||
| TER 6235 ƒe xexlẽdzesi | 33 | 60.6 | 32 | 7.4 | 30 | Ememe tube;Afɔkpa;Foamed akpawo;Sponge profile;Molded nuwɔna | Mooney ƒe ʋeʋẽ si bɔbɔ; Gazazã nyuie; Ethylene si sɔ gbɔ ɖe eme; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dɔwɔwɔ ƒe nunɔamesi nyuitɔ kekeake; ENB ƒe agbɔsɔsɔ si sɔ gbɔ; Dɔyɔyɔ kabakaba; |
||
| TER 6537 ƒe xexlẽdzesi | 43 | 60 | 32 | 8 | 100 | Foamed akpawo;Sponge profile;Klɔmɔ̃ ƒe ʋɔtru nutrenuwo;Molded nuawo | ENB ƒe agbɔsɔsɔ si sɔ gbɔ; Dɔyɔyɔ kabakaba; |
||
| TER 9046 ƒe xexlẽdzesi | 67 | 60.1 | 31 | 8.9 | Foamed akpawo;Sponge profile;Dɔwɔƒewo ƒe nuwɔna | ENB ƒe agbɔsɔsɔ si sɔ gbɔ; Dɔyɔyɔ kabakaba; |
|||
| TER 4548 ƒe xexlẽdzesi | 47 | 59.5 | 36 | 4.5 | 10 | Ememe tube;Afɔkpa;Nu siwo wotsɔ aŋe wɔ ;Dɔwɔƒewo;Nu siwo wotsɔ aŋe wɔe | Mooney ƒe ʋeʋẽ si bɔbɔ; Gazazã nyuie; |
||
| TER 8148 ƒe xexlẽdzesi | 68 | 52.5 | 39 | 8.5 | 21 | Foamed akpawo;Sponge profile;Dɔwɔƒewo ƒe nuwɔna;Molded nuwɔna | Ethylene si mesɔ gbɔ o; ENB ƒe agbɔsɔsɔ si sɔ gbɔ; Dɔyɔyɔ kabakaba; Dzoxɔxɔ ƒe tsitretsitsi si bɔbɔ |
||
| TER 7040 ƒe xexlẽdzesi | 87 | 53.5 | 40 | 6.5 | Hose;Ʋɔtru kple fesre nutrenu strips;Extrusion Product; | Ethylene si mesɔ gbɔ o; Kɔkɔe yɔyɔ; Mooney ƒe ʋeʋẽ lilili si lolo; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo; Dzoxɔxɔ ƒe tsitretsitsi si bɔbɔ |
|||
| TER 4049 ƒe xexlẽdzesi | 76 | 55.5 | 40 | 4.5 | Hose;Ʋɔtru kple fesre nutrenu strips;Extrusion Product; | Ethylene si mesɔ gbɔ o; Dzoxɔxɔ ƒe tsitretsitsi si bɔbɔ |
|||
| TER 5029 ƒe xexlẽdzesi | 80 | 69.5 | 25 | 5.5 | Hose;Ʋɔtru kple fesre nutrenu strips;Extrusion Product; | Kɔkɔe yɔyɔ; Ethylene si sɔ gbɔ ɖe eme; Mooney ƒe ʋeʋẽ lilili si lolo; Mɔ̃ɖaŋununya ƒe nɔnɔme kɔkɔwo |
1. Ʋu ƒe nutrenu ƒe ʋuƒo
Nutrenu strip na hood
Ʋɔtrua ƒe nutrenu
Fesre ƒe screen
Sunroof ƒe nutrenu
Lɔrifɔti ƒe nutrenu
Tsitretsitsi ɖe ke ŋu
Glassrun ƒe mɔ̃a
Tsitretsitsi ɖe toɣliɖeɖe ŋu
2. Hose ƒe ƒuƒoƒo
Brek ƒe hoses
Ʋu ƒe radiator hose
Skylight ƒe tsidzɔƒe ƒe pɔmpi
3. Ka kple ka
Elektrikŋusẽ ƒe ka
Ka si wotsɔ goma blae
Nutoa me kaƒomɔ̃
Television dzi kaƒomɔ̃
Dɔwɔnu ƒe ka
4. Tsi mate ŋu age ɖe eme o ƒe coil
Gli si me tsi mate ŋu age ɖo o ƒe coil
Tame tsi si me tsi mele o ƒe coil
Mɔdodo gã dzi tsi mate ŋu abla agbalẽ xatsaxatsa
Tunnel tsi si me tsi mele o coil
5. Tayawo
Ememe ƒe ʋuƒo
Taya ƒe akpa dzi
Keke ƒe taya
6. Nu dzro siwo wotsɔ aŋe wɔe
Rababa ƒe ʋuƒo
Goma ƒe mat
Gasket si wotsɔ wɔa dɔe
Brek ƒe agba
7. Ami ƒe tɔtrɔ kple agble bubuwo
ami si wotsɔ kpe ɖe eŋu