Telefon: +86 15221953351 E-mail: info@herchyrubber.com
Please Choose Your Language
NUSIWO WOWƆ
Èle afisia: Aƒeme » Nusiwo Wowɔ » Compound

Goma Siwo Wotsɔ Ƒoa Nu: Woƒe Nɔnɔmewo, Viɖewo, Kple Wo Zazã Tsitotsito

1. FKM ƒe Atikewɔwɔ (FKM) .

Nunɔamesiwo:

  • Dzoxɔxɔ ƒe tsitretsitsi si gbɔ eme (-20°C va ɖo +250°C).

  • Tsitretsitsi ɖe ami, dzotsinuwo, atike siwo wotsɔna tsia ami, aɖi, kple amiwo nu etɔxɛe.

  • Tensile ŋusẽ gã (10–20 MPa), low compression ɖoɖo (<15% le 150 ° C / 70h).

  • Dzo si me dzo mele o (UL94 V-0 ƒe dzeside) eye wòte ŋu nɔa te ɖe ozone nu.

Viɖe siwo le eŋu:

  • Wotsɔ atike siwo daa dɔe (le kpɔɖeŋu me, bisphenol AF, peroxide) tsakae do ŋgɔ hena vulcanization nyuie.

  • Eléa didime ƒe liƒo me ɖe asi le atike ƒe nɔnɔme siwo me wowɔa adã le me.

  • Dzeside siwo sɔ ɖe FDA nu li na nuɖuɖu/atikewɔlawo ƒe kadodo.

Dɔwɔwɔwo:

  • Yamenutome: Mɔ̃memi ƒe ɖoɖo ƒe O-rings, mɔ̃a ƒe nutrenu, kple diaphragm.

  • Ʋu: Turbocharger gaskets, ʋu ƒe ʋu ƒe nutrenu, kple mɔ̃memi ƒe mɔ̃wo.

  • Atikewo: Pɔmpi ƒe nutsyɔnu, valvɔ ƒe zikpuiwo, kple hose ƒe ƒuƒoƒo.

2. HNBR ƒe Atike (HNBR) .

Nunɔamesiwo:

  • Dzoxɔxɔ ƒe tsitretsitsi va ɖo +150°C (si nɔa anyi ɣeaɖewoɣi +175°C).

  • Tsitretsitsi ɖe amiwo, aminewo, kple hadrolik tsiwo ŋu nyuie wu.

  • Tensile strength si lolo (15–35 MPa) kple ɖeɖiteameŋu ƒe tsitretsitsi.

  • Yawo ƒe gege ɖe eme si mebɔ o.

Viɖe siwo le eŋu:

  • Do ŋgɔ na vulcanized hena dɔwɔwɔ ƒe ɣeyiɣi dzi ɖeɖe kpɔtɔ.

  • Eléa eƒe elasticity me ɖe asi ne etsɔe de nyadzɔdzɔgblɔmɔ̃ sesẽwo me ɣeyiɣi didi.

  • Woate ŋu akpɔe le peroxide- alo sulphur-cured ƒe hatsotsowo me.

Dɔwɔwɔwo:

  • Ami Kple Gas: Domenuwo ƒe nudzraɖoƒewo, anyikpe pɔmpi ƒe nutrenuwo, kple vudo ƒe ta ƒe akpa aɖewo.

  • Ʋuwo: Ɣeyiɣidzidzenu, mɔ̃memi dodo ƒe mɔ̃wo, kple turbocharger hoses.

  • Dɔwɔƒewo: Haidrɔlik tsilindo ƒe nutrenuwo kple gearbox ƒe akpa aɖewo.

3. NBR ƒe Atike (NBR) .

Nunɔamesiwo:

  • Ami ƒe tsitretsitsi si sɔ (enyo wu EPDM, mede HNBR nu o).

  • Dzoxɔxɔ ƒe didime: -40°C va ɖo +120°C.

  • Tsitretsitsi ɖe ʋuʋudedi ŋu si lolo (ASTM D5963: 100–200 mm3 ƒe bu).

  • Tenɔnɔ ɖe nɔnɔme sesẽwo nu nyuie kple nutete ɖo tsitretsitsi.

Viɖe siwo le eŋu:

  • Gazazã nyuie kple moldability nyuitɔ kekeake.

  • Acrylonitrile ƒe agbɔsɔsɔ si woate ŋu atrɔ asi le (18–50%) na ami ƒe tsitretsitsi si wowɔ ɖe ɖoɖo nu.

Dɔwɔwɔwo:

  • Ʋu: Mɔ̃memi ƒe hoses, O-rings, kple transmission seals.

  • Dɔwɔƒewo: Alidziblanu siwo wotsɔna tsɔa nu, agbalẽtata ƒe agbalẽ xatsaxatsawo, kple hadrolik-nutrenuwo.

  • Nuƒlela: Latex-asigɛwo kple kamedefefewɔnuwo.

4. EPDM ƒe Atike (Ethylene Propylene Diene Monomer) .

Nunɔamesiwo:

  • Ozone/yame ƒe nɔnɔme ƒe tsitretsitsi ɖedzesi aɖe (gaƒoƒo 5,000+ le QUV dodokpɔ me).

  • Dzoxɔxɔ ƒe didime: -50°C va ɖo +150°C.

  • Dielectric ŋusẽ gã (20–30 kV/mm) kple tsi ƒe gege ɖe eme.

  • Gas ƒe gege ɖe eme si mebɔ o.

Viɖe siwo le eŋu:

  • Wotsɔ antioxidants kple UV stabilizers wɔe do ŋgɔ.

  • Vibration damping nyuitɔ kekeake (nubuname ƒe akpa: 0.1–0.3).

Dɔwɔwɔwo:

  • Ʋu: Ʋɔtru ƒe nutrenuwo, radiator hosewo, kple mɔ̃a ƒe mɔ̃wo.

  • Xɔtutu: Tame ƒe lãkusiwo, tsita ƒe nutrenuwo, kple fesre ƒe gazewo.

  • Elektrikŋusẽ: Ka siwo wotsɔ xea mɔ na dzoxɔxɔ kple elektrikŋusẽ ƒe alidziblanu.

5. MPU ƒe Atikewɔwɔ (MPU) .

Nunɔamesiwo:

  • Tensile ŋusẽ si lolo (20–60 MPa) kple elasticity (vaseɖe 800% didime).

  • Tsitretsitsi ɖe ʋuʋudedi ŋu etɔxɛe (ASTM D5963: 20–50 mm3 ƒe bu).

  • Dzoxɔxɔ ƒe didime: -40°C va ɖo +100°C (va ɖo +120°C kple dzoxɔxɔdzidzenuwo).

  • Ete ŋu nɔa te ɖe atike siwo wotsɔna tsia ami nu kple tsi ƒe ʋuʋu nu.

Viɖe siwo le eŋu:

  • Sesẽme si woate ŋu atrɔ asi le (Shore A 50–95).

  • Woate ŋu akpɔe le cast, millable, alo thermoplastic ƒe hatsotsowo me.

Dɔwɔwɔwo:

  • Dɔwɔƒewo: Tasiaɖamfɔwo, agbalẽ xatsaxatsawo, kple mɔ̃ siwo wotsɔna tsɔa nu.

  • Ʋu: Afɔkpa siwo wotsɔna tsia ʋuae, afɔkpa siwo xea mɔ na ʋu, kple CV joint boots.

  • Atikewɔwɔ: Catheters, ƒunukpeƒetetedɔ, kple ƒumeŋuɖui.

6. ACM ƒe Atikewɔwɔ (ACM) .

Nunɔamesiwo:

  • Dzoxɔxɔ ƒe tsitretsitsi atraɖii va ɖo +150°C (si nɔa anyi ɣeaɖewoɣi +175°C).

  • Tsitretsitsi ɖe tsi siwo wotsɔna ʋua mɔ̃memi le wo ɖokui si (ATF), amiwo, kple dzoxɔxɔ ŋu nyuie ŋutɔ.

  • Ozone kple yame ƒe nɔnɔme ƒe tsitretsitsi si sɔ.

  • Ŋusẽ si wotsɔna ƒoa nu: 7-15 MPa.

Viɖe siwo le eŋu:

  • Wotsɔa amine alo peroxide ƒe atikewo tsakana do ŋgɔ be wòada gbe le eŋu kabakaba.

  • Eléa didime ƒe liƒo me ɖe asi le ATF nɔnɔmewo me.

Dɔwɔwɔwo:

  • Ʋu: Ʋuɖoɖo ƒe nutrenu, O-ring, kple pɔmpi ƒe ʋuƒo.

  • Power steering system ƒe akpa aɖewo.

  • Dɔwɔƒewo: Pɔmpi ƒe nutrenuwo na nyadzɔdzɔgblɔmɔ̃ siwo me ami le.

7. AEM ƒe Atikewɔwɔ (AEM) .

Nunɔamesiwo:

  • Dzoxɔxɔ ƒe didime si keke ta (-40°C va ɖo +150°C).

  • Tsitretsitsi ɖe amiwo, glycols, kple yame ƒe nɔnɔme ƒe tɔtrɔ ŋu.

  • Kɔkɔ tensile ŋusẽ (10–20 MPa) kple compression ɖoɖo tsitretsitsi.

  • Yawo ƒe gege ɖe eme si mebɔ o.

Viɖe siwo le eŋu:

  • Edaa dzoxɔxɔ ƒe tsitretsitsi kple asitɔtrɔ le nɔnɔmewo ŋu.

  • Ete ŋu nɔa te ɖe tsi ƒe ʋuʋu kple tsitsi nu.

  • Woate ŋu akpɔe le peroxide- alo sulphur-cured ƒe hatsotsowo me.

Dɔwɔwɔwo:

  • Ʋu: Radiator hoses, fafamɔ̃ ƒe akpa aɖewo, kple yaxɔƒe hoses.

  • Dɔwɔƒewo: Conveyor belts na atikewo zazã kple pɔmpi diaphragms.

  • HVAC: Duct gaskets kple vibration isolators.


NYAWO ƑE ƑOMEDODO KABA

MÍAƑE NUWO ƑE NUWO

NYATAKAKA SIWO WOÐO BE WOAÐO BE WOAÐE KPƆKPƆ

Tsɔ kpe ɖe eŋu: No.33, Mɔdodo 159, Taiye Mɔ dzi, Fengxian Nutome, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nutata ƒe Gomenɔamesi     2023 Shanghai Herchy Rubber Co., Ltd. Nyatakakadzraɖoƒe ƒe Nɔnɔmetata |   Ameŋunyatakakawo Ŋuti Ðoɖo | Kpekpeɖeŋu To Leadong ƒe agbalẽ.