GA-11×1
Herchy
| Ho fumaneha: | |
|---|---|
| Bongata: | |
Teko: 1% ea moemeli oa phekolo (50% peista ea DBPMH ka silicone gum), 175 ° x 5min x 15MPa.
| Lihlahisoa tsa lihlahisoa | ||||||
| Sehlahisoa | GA-11331 |
GA-1141 | GA-1151 | GA-1161 | GA-1171 | GA-1181 |
| Ponahalo | Translucent | |||||
| Williamplasticity |
115 |
150 |
205 |
240 |
280 |
260 |
| Ho thatafala (LebopoA) |
30 |
40 |
50 |
60 |
70 |
80 |
| Boima ba 'mele(g/cm3) | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.23 |
| Tensilestrength (MPa) |
7 |
8.5 |
8.5 |
8.5 |
7.5 |
7.5 |
| Elongation(%) | 700 |
550 |
450 |
400 |
300 |
200 |
| Matla a metsi (kN/m) | 15 |
19 |
20 |
19 |
19 |
19 |