GA-11 × 1
Herchy
| Muaj: | |
|---|---|
| Quantity: | |
Kev kuaj: 1% ntawm tus neeg saib xyuas (50% muab tshuaj txhuam ntawm DBPMH hauv cov pos hniav silicone), 175 ° x 5min x 15MPa.
| Khoom parameters | ||||||
| Khoom | TIAB SA-11331 |
TIAB SA-1141 | TIAB SA-1151 | TIAB SA-1161 | TIAB SA-1171 | TIAB SA-1181 |
| Qhov tshwm sim | Translucent | |||||
| Williamplasticity |
115 |
150 |
205 |
240 |
280 |
260 |
| Hardness (ShoreA) |
30 |
40 |
50 |
60 |
70 |
80 |
| Qhov ceev (g / cm3) | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.23 |
| Tensilestrength (MPa) |
7 |
8.5 |
8.5 |
8.5 |
7.5 |
7.5 |
| Elongation (%) | 700 |
550 |
450 |
400 |
300 |
200 |
| Siab zog (kN / m) | 15 |
19 |
20 |
19 |
19 |
19 |