GA-11×1
Herchy
| Availability: | |
|---|---|
| Dami: | |
Pagsubok: 1% ng curing agent (50% paste ng DBPMH sa silicone gum),175° x 5min x 15MPa.
| Mga parameter ng produkto | ||||||
| produkto | GA-11331 |
GA-1141 | GA-1151 | GA-1161 | GA-1171 | GA-1181 |
| Hitsura | Translucent | |||||
| Williamplasticity |
115 |
150 |
205 |
240 |
280 |
260 |
| Katigasan (ShoreA) |
30 |
40 |
50 |
60 |
70 |
80 |
| Densidad(g/cm3) | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.23 |
| Tensilstrength (MPa) |
7 |
8.5 |
8.5 |
8.5 |
7.5 |
7.5 |
| Pagpahaba(%) | 700 |
550 |
450 |
400 |
300 |
200 |
| Lakas ng luha (kN/m) | 15 |
19 |
20 |
19 |
19 |
19 |