GA-11×1
Herchy
| Beskikberens: | |
|---|---|
| Quantity: | |
Test: 1% kurermiddel (50% pasta fan DBPMH yn silikongom), 175 ° x 5min x 15MPa.
| Produkt parameters | ||||||
| Produkt | GA-11331 |
GA-1141 | GA-1151 | GA-1161 | GA-1171 | GA-1181 |
| Ferskining | Trochsichtich | |||||
| Williamplasticity |
115 |
150 |
205 |
240 |
280 |
260 |
| Hardheid (ShoreA) |
30 |
40 |
50 |
60 |
70 |
80 |
| Tichtheid (g/cm3) | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.23 |
| Treksterkte (MPa) |
7 |
8.5 |
8.5 |
8.5 |
7.5 |
7.5 |
| Ferlinging (%) | 700 |
550 |
450 |
400 |
300 |
200 |
| Tearsterkte (kN/m) | 15 |
19 |
20 |
19 |
19 |
19 |